Correlation between friction-induced microstructural evolution, strain hardening in subsurface and tribological properties of AZ31 magnesium alloy

被引:55
作者
Liang, C. [1 ]
Li, C. [1 ]
Lv, X. X. [1 ]
An, J. [1 ]
机构
[1] Jilin Univ, Dept Mat Sci & Engn, Minist Educ, Key Lab Automobile Mat, Changchun 130025, Peoples R China
关键词
Sliding wear; Non-ferrous metals; Hardness; Wear testing; Surface analysis; Wear modeling; SLIDING WEAR BEHAVIOR; PLASTIC-DEFORMATION;
D O I
10.1016/j.wear.2014.02.001
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Dry sliding tests were performed on as-cast AZ31 magnesium alloy using a pin-on-disc configuration. Coefficients of friction and wear rates were measured within a load range of 5-360 N and a sliding velocity range of 0.1-4.0 m/s. Morphologies, compositions and hardness of worn surfaces were characterized by scanning electron microscope (SEM), energy dispersive X-ray spectrometer (EDS) and hardness tester. Microstructural evolution, strain hardening and dynamic crystallization (DRX) generated in subsurfaces of AZ31 alloy during sliding were found to correlate with the tribological properties obtained. The subsurface microstructures beneath the contact surface were subjected to large plastic strains, and experienced strain hardening, DRX and melting as a result. The roles of surface hardening and thermal softening on the mild to severe wear transition were investigated in detail. It was shown that the transition occurred when the surface layer softened with DRX. Surface oxidation and strain hardening played an important role in maintaining the mild wear, and thermal softening originating from DRX in subsurface and surface melting were responsible for the severe wear. A transition load model, which can be used predict the critical load for transition from mild to severe wear, has been developed using the method of DRX kinetics. A map has been constructed for presenting microstructural evolution and hardness change in surface layer based on the calculated mild to severe wear transition loads and critical loads for surface melting. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:29 / 39
页数:11
相关论文
共 25 条
[1]   Dry sliding wear behavior of magnesium alloys [J].
An, J. ;
Li, R. G. ;
Lu, Y. ;
Chen, C. M. ;
Xu, Y. ;
Chen, X. ;
Wang, L. M. .
WEAR, 2008, 265 (1-2) :97-104
[2]   Wear behaviour of a Mg alloy subjected to friction stir processing [J].
Arora, H. S. ;
Singh, H. ;
Dhindaw, B. K. .
WEAR, 2013, 303 (1-2) :65-77
[3]  
Avedesian M.M., 1999, MAGNESIUM MAGNESIUM
[4]   Influence of grain size on the compressive deformation of wrought Mg-3Al-1Zn [J].
Barnett, MR ;
Keshavarz, Z ;
Beer, AG ;
Atwell, D .
ACTA MATERIALIA, 2004, 52 (17) :5093-5103
[5]  
Blawert C, 2004, T INDIAN I METALS, V57, P397
[6]   Sliding wear map for the magnesium alloy Mg-9Al-0.9 Zn (AZ91) [J].
Chen, H ;
Alpas, AT .
WEAR, 2000, 246 (1-2) :106-116
[7]   Microstructural evolution during high temperature sliding wear of Mg-3% Al-1% Zn (AZ31) alloy [J].
Das, S. ;
Morales, A. T. ;
Alpas, A. T. .
WEAR, 2010, 268 (1-2) :94-103
[8]   Sliding temperature and wear behaviour of cast Al-Si-Mg alloys [J].
Dwivedi, DK .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 382 (1-2) :328-334
[9]   Tribological behavior of pure Mg and AZ31 magnesium alloy strengthened by Al2O3 nano-particles [J].
Habibnejad-Korayem, M. ;
Mahmudi, R. ;
Ghasemi, H. M. ;
Poole, W. J. .
WEAR, 2010, 268 (3-4) :405-412
[10]   The elevated-temperature mechanical behavior of peak-aged Mg-10Gd-3Y-0.4Zr Alloy [J].
Janik, V. ;
Yin, D. D. ;
Wang, Q. D. ;
He, S. M. ;
Chen, C. J. ;
Chen, Z. ;
Boehlert, C. J. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (7-8) :3105-3112