In vitro and in vivo studies of biodegradable fine grained AZ31 magnesium alloy produced by equal channel angular pressing

被引:114
作者
Sunil, B. Ratna [1 ]
Kumar, T. S. Sampath [1 ]
Chakkingal, Uday [1 ]
Nandakumar, V. [2 ]
Doble, Mukesh [2 ]
Prasad, V. Devi [3 ]
Raghunath, M. [3 ]
机构
[1] Indian Inst Technol, Dept Met & Mat Engn, Madras 600036, Tamil Nadu, India
[2] Indian Inst Technol, Dept Biotechnol, Madras 600036, Tamil Nadu, India
[3] NTR Coll Vet Sci, Dept Surg & Radiol, Gannavaram 521102, India
来源
MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS | 2016年 / 59卷
关键词
Magnesium; Ultra fine grains; AZ31 Mg alloy; Biodegradation; ECAP; Wettability; SIMULATED BODY-FLUID; NANOCRYSTALLINE MATERIALS; MG ALLOYS; CORROSION; COATINGS; DEGRADATION; RESISTANCE; BEHAVIOR; BIOMATERIALS; IMPLANTS;
D O I
10.1016/j.msec.2015.10.028
中图分类号
TB3 [工程材料学]; R318.08 [生物材料学];
学科分类号
0805 ; 080501 ; 080502 ;
摘要
The objective of the present work is to investigate the role of different grain sizes produced by equal channel angular pressing (ECAP) on the degradation behavior of magnesium alloy using in vitro and in vivo studies. Commercially available AZ31 magnesium alloy was selected and processed by ECAP at 300 degrees C for up to four passes using route B-c. Grain refinement from a starting size of 46 pm to a grain size distribution of 1-5 mu m-was Successfully achieved after the 4th pass. Wettability of ECAPed samples assessed by contact angle measurements was found to increase due to the fine grain structure. In vitro degradation and bioactivity of the samples studied by immersing in super saturated simulated body fluid (SBF 5 x) showed rapid mineralization within 24 h due to the increased wettability in fine grained AZ31 Mg alloy. Corrosion behavior of the samples assessed by weight loss and electrochemical tests conducted in SBF 5 x clearly showed the prominent role of enhanced mineral deposition on ECAPed AZ31 Mg in controlling the abnormal degradation. Cytotoxicity studies by MIT colorimetric assay showed that all the samples are viable. Additionally, cell adhesion was excellent for ECAPed samples particularly for the 3rd and 4th pass samples. In vivo experiments conducted using New Zealand White rabbits clearly showed lower degradation rate for ECAPed sample compared with annealed AZ31 Mg alloy and all the samples showed biocompatibility and no health abnormalities were noticed in the animals after 60 days of in vivo studies.. These results suggest that the grain size plays an important role in degradation management of magnesium alloys and ECAP technique can be adopted to achieve fine grain structures for developing degradable magnesium alloys for biomedical applications. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:356 / 367
页数:12
相关论文
共 47 条
[22]   Critical discussion of the results from different corrosion studies of Mg and Mg alloys for biomaterial applications [J].
Mueller, Wolf-Dieter ;
Nascimento, M. Lucia ;
Fernandez Lorenzo de Mele, Monica .
ACTA BIOMATERIALIA, 2010, 6 (05) :1749-1755
[23]   Rapid coating of AZ31 magnesium alloy with calcium deficient hydroxyapatite using microwave energy [J].
Ren, Yufu ;
Zhou, Huan ;
Nabiyouni, Maryam ;
Bhaduri, Sarit B. .
MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2015, 49 :364-372
[24]   HARDNESS GRAIN-SIZE RELATIONS IN CERAMICS [J].
RICE, RW ;
WU, CC ;
BORCHELT, F .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (10) :2539-2553
[25]   Calcium phosphate coatings on magnesium alloys for biomedical applications: A review [J].
Shadanbaz, Shaylin ;
Dias, George J. .
ACTA BIOMATERIALIA, 2012, 8 (01) :20-30
[26]   A study of strontium doped calcium phosphate coatings on AZ31 [J].
Singh, Satish S. ;
Roy, Abhijit ;
Lee, Boeun E. ;
Ohodnicki, John ;
Loghmanian, Autrine ;
Banerjee, Ipsita ;
Kumta, Prashant N. .
MATERIALS SCIENCE AND ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2014, 40 :357-365
[27]   Corrosion behavior of equal-channel-angular-pressed pure magnesium in NaCl aqueous solution [J].
Song, Dan ;
Ma, AiBin ;
Jiang, Jinghua ;
Lin, Pinghua ;
Yang, Donghui ;
Fan, Junfeng .
CORROSION SCIENCE, 2010, 52 (02) :481-490
[28]   Biodegradable behaviors of AZ31 magnesium alloy in simulated body fluid [J].
Song, Yingwei ;
Shan, Dayong ;
Chen, Rongshi ;
Zhang, Fan ;
Han, En-Hou .
MATERIALS SCIENCE & ENGINEERING C-BIOMIMETIC AND SUPRAMOLECULAR SYSTEMS, 2009, 29 (03) :1039-1045
[29]   Magnesium and its alloys as orthopedic biomaterials: A review [J].
Staiger, MP ;
Pietak, AM ;
Huadmai, J ;
Dias, G .
BIOMATERIALS, 2006, 27 (09) :1728-1734
[30]   Processing and mechanical behavior of lamellar structured degradable magnesium-hydroxyapatite implants [J].
Sunil, B. Ratna ;
Ganapathy, C. ;
Kumar, T. S. Sampath ;
Chakkingal, Uday .
JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2014, 40 :178-189