Influence of carbon sources on nitriding process, microstructures and mechanical properties of Si3N4 bonded SiC refractories

被引:18
作者
Chen, Junfeng [1 ]
Li, Nan [1 ]
Wei, Yaowu [1 ]
Han, Bingqiang [1 ]
Yan, Wen [1 ]
机构
[1] Wuhan Univ Sci & Technol, Key State Lab Refractories & Met, Wuhan 430081, Peoples R China
基金
中国国家自然科学基金;
关键词
Nitridation degree; Carbon; Microstructure; Thermal shock resistance; SILICON-NITRIDE; CERAMICS; OXIDATION; ADDITIVES; WHISKERS;
D O I
10.1016/j.jeurceramsoc.2016.12.005
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The incomplete nitriding and heterogeneity structure of large-size Si3N4-bonded SiC refractories limited its application in refractories industry. The objective of this work was to provide a way that adding carbon in matrix with the expectations of carbon could reacted with free-Si and transformed into SiC after nitridation. The effects of carbon sources on the bonded morphologies and nitridation process of Si3N4 bonded SiC refractories were investigated. Results indicated the strength and Young's-modulus of specimen with carbon black increased to 39.4 MPa and 103.89 GPa from 29.8 MPa and 73.43 GPa, respectively. The residual Young's-modulus also improved from 44.13 GPa to 62.9 GPa after 9-quenching cycles. For specimen with graphite, residual graphite after nitridation resulted in a definite strength decline, but residual strength after quenching was improved. Moreover, analysis results on N-elements indicated surprisingly improvement in the nitriding degree for specimen with carbon black. The microstructure evolution and mechanism associating with the enhanced nitriding process was discussed. (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1821 / 1829
页数:9
相关论文
共 50 条
[21]   Fabrication, mechanical properties and microstructure analysis of Si3N4/SiC nanocomposite [J].
Cheong, DS ;
Hwang, KT ;
Kim, CS .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 1999, 30 (04) :425-427
[22]   Effects of β-Si3N4 Seeds Addition on Microstructure and Mechanical Properties of Porous Si3N4 Ceramics [J].
Yu, Fang-li ;
Bai, Yu ;
Du, Jun ;
Yu, Ping-ping ;
Wang, Jian-zhi ;
Yang, Jian-feng .
ECO-MATERIALS PROCESSING AND DESIGN XIII, 2012, 724 :201-+
[23]   Fabrication, mechanical properties and thermal shock resistance of a dense SiC NWs/α-Si3N4 composite coating for protecting porous Si3N4 ceramics [J].
Wang, Binglei ;
Shangguan, Duandan ;
Qiao, Ruiqing ;
Zhang, Fan ;
Bai, Yu ;
Wang, Zhanjie ;
Wang, Chao ;
Lu, Xuefeng .
CERAMICS INTERNATIONAL, 2019, 45 (17) :23241-23247
[24]   Effects of Microwave Sintering Temperature and Holding Time on Mechanical Properties and Microstructure of Si3N4/n-SiC ceramics [J].
Qiao, Li ;
Wang, Zhenhua ;
Lu, Taiyi ;
Yuan, Juntang .
MATERIALS, 2019, 12 (23)
[25]   Influence of grinding parameters on Si3N4 ceramic mechanical properties [J].
Rodriguez, R ;
Leriche, A ;
Carrerot, H .
SILICATES INDUSTRIELS, 2004, 69 (7-8) :325-332
[26]   Microstructure and mechanical properties of an Si3N4/Si3N4 joint brazed with Au-Ni-Pd-V filler alloy [J].
Sun, Y. ;
Zhang, J. ;
Geng, Y. P. ;
Ikeuchi, K. ;
Shibayanagi, T. .
SCRIPTA MATERIALIA, 2011, 64 (05) :414-417
[27]   Mechanical properties of Si3N4 ceramics from an in-situ synthesized a-Si3N4/β-Si3N4 composite powder [J].
Xing, Hongyu ;
Liu, Bingqiang ;
Sun, Jing ;
Zou, Bin .
CERAMICS INTERNATIONAL, 2017, 43 (02) :2150-2154
[28]   Fabrication and mechanical properties of in-situ Si3N4 bonded MgO-C refractories by nitrogen gas pressure sintering [J].
Cheng, Xu ;
Yu, Chao ;
Xing, Guang-chao ;
Ma, Bei-yue ;
Ding, Jun ;
Wang, Zhou-fu ;
Zhang, Ji-xiang ;
Zhu, Hong-xi ;
Deng, Cheng-ji .
JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2025, 32 (07) :2016-2026
[29]   Influence of SiC particle size on creep properties of Si3N4/SiC composite ceramics [J].
Sato, S ;
Chu, MC ;
Kobayashi, Y ;
Ando, K .
JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1996, 104 (11) :1035-1039
[30]   Friction and wear properties of SiC and Si3N4 in emulsion lubrication [J].
Hironaka, S ;
Kawamura, D ;
Suzuki, M .
JOURNAL OF JAPANESE SOCIETY OF TRIBOLOGISTS, 2003, 48 (06) :486-493