Oxidation Characteristics and Oxide Layer Evolution of Alloy 617 and Haynes 230 at 900 A°C and 1100 A°C

被引:137
作者
Kim, Daejong [1 ]
Jang, Changheui [1 ]
Ryu, Woo Seog [2 ]
机构
[1] Korea Adv Inst Sci & Technol, Dept Nucl & Quantum Engn, Taejon 305701, South Korea
[2] Korea Atom Energy Res Inst, Nucl Mat Technol Dev Div, Taejon 305600, South Korea
来源
OXIDATION OF METALS | 2009年 / 71卷 / 5-6期
关键词
Oxidation characteristics; Oxide layer evolution; Spallation; Alloy; 617; Haynes; 230; HIGH-TEMPERATURE CORROSION; NICKEL-BASE ALLOY; HELIUM ENVIRONMENTS; IMPURE HELIUM; KINETICS; AIR; INCONEL-617; IMPURITIES; RESISTANCE; BEHAVIOR;
D O I
10.1007/s11085-009-9142-5
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
To evaluate the oxidation resistance of Alloy 617 and Haynes 230, oxidation tests were performed at 900 A degrees C and 1100 A degrees C in air and helium environments. Scale characterizations were assessed on specimens exposed to air using thin-film XRD, XPS, SEM and EDX. Oxidation resistance was dependent on the stability of the surface oxide layer, which can be affected by minor alloying elements such as Ti and Mn. At 900 A degrees C, for Alloy 617, a mixture of the extensive NiO-Cr2O3 double layer and isolated NiO-NiCr2O4-Cr2O3 triple layer were observed at a steady-state condition. For Haynes 230, a MnCr2O4 layer was formed on top of the Cr2O3 layer, resulting in a lower oxidation rate. At 1100 A degrees C, both alloys showed a double layer consisting of an inner Cr2O3 and outer MnCr2O4 or TiO2. The spallation of outer layer and subsequent volatilization of the Cr2O3 layer produced a rugged surface and interface as well as internal oxidation.
引用
收藏
页码:271 / 293
页数:23
相关论文
共 26 条
  • [1] LONG-TERM OXIDATION OF SUPERALLOYS
    ANGERMAN, CL
    [J]. OXIDATION OF METALS, 1972, 5 (02): : 149 - 167
  • [2] [Anonymous], 2003, MAT BEHAV HTGR ENV
  • [3] RESISTANCE OF NI-CR-AL ALLOYS TO CYCLIC OXIDATION AT 1100 AND 1200-DEGREES-C
    BARRETT, CA
    LOWELL, CE
    [J]. OXIDATION OF METALS, 1977, 11 (04): : 199 - 223
  • [4] Birks N., 2006, INTRO HIGH TEMPERATU
  • [5] High temperature reactivity of two chromium-containing alloys in impure helium
    Cabet, C.
    Chapovaloff, J.
    Rouillard, F.
    Girardin, G.
    Kaczorowski, D.
    Wolski, K.
    Pijolat, M.
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2008, 375 (02) : 173 - 184
  • [6] HIGH-TEMPERATURE CORROSION OF THE NICKEL-BASED ALLOY INCONEL-617 IN HELIUM CONTAINING SMALL AMOUNTS OF IMPURITIES
    CHRIST, HJ
    KUNECKE, U
    MEYER, K
    SOCKEL, HG
    [J]. MATERIALS SCIENCE AND ENGINEERING, 1987, 87 (1-2): : 161 - 168
  • [7] EFFECT OF CR2O3 VOLATILIZATION ON OXIDATION KINETICS OF A NI-CR ALLOY
    ECER, GM
    MEIER, GH
    [J]. SCRIPTA METALLURGICA, 1973, 7 (11): : 1189 - 1194
  • [8] Oxidation kinetics of some nickel-based superalloy foils and electronic resistance of the oxide scale formed in air Part I
    England, DM
    Virkar, AV
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1999, 146 (09) : 3196 - 3202
  • [9] GLEESON B, 2001, P EFC WORKSH, V34, P167
  • [10] CORROSION OF METALLIC MATERIALS IN HTR-HELIUM ENVIRONMENTS
    GRAHAM, LW
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1990, 171 (01) : 76 - 83