Improving sliding and abrasive wear behaviour of cast A356 and wrought AA7075 aluminium alloys by plasma electrolytic oxidation

被引:90
|
作者
Sabatini, G. [1 ]
Ceschini, L. [1 ]
Martini, C. [1 ]
Williams, J. A. [2 ]
Hutchings, I. M. [3 ]
机构
[1] Univ Bologna, SMETEC Dept, I-40136 Bologna, Italy
[2] Univ Cambridge, Dept Engn, Cambridge CB2 1PZ, England
[3] Univ Cambridge, Inst Mfg, Cambridge CB2 1RX, England
关键词
Non-ferrous metals and alloys; Surface treatments; Wear; TRIBOLOGICAL BEHAVIOR; MICROARC OXIDATION; OXIDE COATINGS; MECHANISMS; MICROSTRUCTURE;
D O I
10.1016/j.matdes.2009.07.053
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
An important limitation of aluminium alloys for mechanical applications is their poor tribological behaviour. In this study, surface treatment by plasma electrolytic oxidation (PEO) has been applied to two widely used aluminium alloys: A359 (hypoeutectic Al-Si-Mg) cast alloy and AA7075 (Al-Zn-Mg-Cu) wrought alloy, in order to improve their wear resistance, under sliding and abrasive wear conditions. The main aim of this work was the comparison of the properties and wear resistance of the oxide layers grown under the same PEO treatment conditions on two different aluminium alloys which might be coupled in engineered components. Significant differences in the phase composition, microstructure and mechanical properties measured by microindentation were observed in the oxide layers grown on the two substrates, and were ascribed to the effects of the different compositions and microstructures of the substrate alloys. Abrasion tests were carried out in a micro-scale abrasion (ball-cratering) test, with both alumina and silicon carbide abrasive particles. The results demonstrated the influence of the abrasive material on wear behaviour: whereas relatively aggressive Sic particles gave comparable results for both PEO treated and untreated samples, with the less aggressive Al2O3 abrasive the wear rates of the PEO treated samples, for both substrates, were significantly lower than those of the untreated substrates. In unlubricated sliding the PEO treatment significantly increase the wear resistance of both the aluminium alloys, at low applied load. In this condition the wear behaviour of the PEO treated alloys is strongly influenced by the stability of a protective Fe-O transfer layer, generated by wear damage of the steel counterpart. Under high applied loads however, the transfer layer is not stable and the hardness of the PEO layer, as well as the load bearing capacity of the substrate, become the main factors in influencing wear resistance. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:816 / 828
页数:13
相关论文
共 44 条
  • [1] The influences of ECAP on the dry sliding wear behaviour of AA7075 aluminium alloy
    Avcu, Egemen
    TRIBOLOGY INTERNATIONAL, 2017, 110 : 173 - 184
  • [2] Sliding wear behaviour of plasma electrolytic oxidation coating on pure aluminium
    Jiang, Yongfeng
    Zhang, Yingyue
    Bao, Yefeng
    Yang, Ke
    WEAR, 2011, 271 (9-10) : 1667 - 1670
  • [3] Improving wear and corrosion properties of alumina coating on AA7075 aluminum by plasma electrolytic oxidation: Effects of graphite absorption
    Haghighat-Shishavan, Babak
    Azari-Khosrowshahi, Rasoul
    Haghighat-Shishavan, Safa
    Nazarian-Samani, Masoud
    Parvini-Ahmadi, Naghi
    APPLIED SURFACE SCIENCE, 2019, 481 : 108 - 119
  • [4] Abrasive and Sliding Wear Characteristics of Al-Si Cast Alloys Before and After Coating by Plasma Electrolytic Oxidation Process
    Aydin, Hakan
    Bayram, Ali
    Uguz, Agah
    MATERIALS TESTING-MATERIALS AND COMPONENTS TECHNOLOGY AND APPLICATION, 2008, 50 (06): : 318 - 325
  • [5] Development of thermal control coatings on AA7075 by plasma electrolytic oxidation (PEO) process
    Ramakrishnan, E.
    Premchand, C.
    Manojkumar, P.
    Rameshbabu, N.
    MATERIALS TODAY-PROCEEDINGS, 2021, 46 : 1085 - 1090
  • [6] An Examination on Dry Sliding Wear Behaviour of AA7075 Aluminium Alloy Modified with FA/Cu Electro-Discharge Coating
    Uthirapathi E.
    Chinnamuthu S.
    Kaliyamoorthi N.
    Journal of Bio- and Tribo-Corrosion, 2024, 10 (02)
  • [7] Aluminium Silicate Concentration and Coordination effect with Tungsten sulphide improving Dry Sliding Wear Characteristics of AA7075 alloy Composites
    P. Loganathan
    K. Rajkumar
    A. Gnanavelbabu
    K. Vishal
    Silicon, 2022, 14 : 12615 - 12631
  • [8] Aluminium Silicate Concentration and Coordination effect with Tungsten sulphide improving Dry Sliding Wear Characteristics of AA7075 alloy Composites
    Loganathan, P.
    Rajkumar, K.
    Gnanavelbabu, A.
    Vishal, K.
    SILICON, 2022, 14 (18) : 12615 - 12631
  • [9] Sliding wear behaviour of electrolytic plasma nitrided cast iron and steel
    Nie, X
    Wang, L
    Yao, ZC
    Zhang, L
    Cheng, F
    SURFACE & COATINGS TECHNOLOGY, 2005, 200 (5-6): : 1745 - 1750
  • [10] Influence of Plasma Electrolytic Oxidation of Cast Al-Si Alloys on Their Phase Composition and Abrasive Wear Resistance
    Student, Mykhailo
    Pohrelyuk, Iryna
    Padgurskas, Juozas
    Posuvailo, Volodymyr
    Hvozdets'kyi, Volodymyr
    Zadorozhna, Khrystyna
    Chumalo, Halyna
    Veselivska, Halyna
    Kovalchuk, Ihor
    Kychma, Andrii
    COATINGS, 2023, 13 (03)