Hot Corrosion Behavior of Si-Y-Co-Modified Aluminide Coating Exposed to NaCl + Na2SO4 Salt at 1173 K

被引:11
|
作者
Liu, Zongjie [1 ]
Zhou, Chungen [1 ]
机构
[1] Beijing Univ Aeronaut & Astronaut, Sch Mat Sci & Engn, Key Lab Aerosp Mat & Performance, Minist Educ, Beijing 100191, Peoples R China
来源
OXIDATION OF METALS | 2016年 / 85卷 / 1-2期
基金
中国国家自然科学基金;
关键词
Metal coatings; Superalloys; Hot corrosion; CYCLIC OXIDATION BEHAVIOR; PHASE-TRANSFORMATIONS; SILICON; RESISTANCE; ALLOY; PACK; AL;
D O I
10.1007/s11085-015-9599-3
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The microstructure and hot corrosion behavior of a Si-Y-Co-modified aluminide coating prepared on a nickel base superalloy DZ125 by the pack cementation process was studied. The Co-Al-Si-Y coated specimen had a mass gain of only 0.25 mg/cm(2) after being exposed to NaCl + Na2SO4 salt for 100 h at 1173 K. Thus the addition of Si to a Y-Co-modified aluminide coating increased its hot corrosion resistance by 40 %. The improved hot corrosion resistance of the Co-Al-Si-Y coating was mainly attributed to the formation of an Al2O3 scale with SiO2 on the surface of the coating during the hot corrosion test. SiO2 can prohibit the high fluxing rate of dissolution of the protective Al2O3 scale and prevent rapid corrosion attack owing to its low solubility over a wide range of salt acidity and its weak oxygen permeability. Graphical Abstract The Co-Al-Si-Y coated specimen had a mass gain of only 0.25 mg/cm(2) after being exposed to NaCl + Na2SO4 salt for 100 h at 1173 K. The addition of Si to a Y-Co-modified aluminide coating improved its hot corrosion resistance. [GRAPHICS]
引用
收藏
页码:205 / 217
页数:13
相关论文
共 50 条
  • [31] Study of hot corrosion resistance of electroless nickel coating with different content of phosphorous in molten salt deposit Na2SO4–NaCl at 650°C
    Ghaderi M.
    Rezagholizadeh M.
    Nasiri-Vatan H.
    Ebrahimi-Kahrizsangi R.
    Surface Engineering and Applied Electrochemistry, 2015, 51 (04) : 367 - 373
  • [32] Hot corrosion behaviour of a Ni plus CrAlYSiN composite coating in Na2SO4-25 wt.% NaCl melt
    Zhu, Lijuan
    Zhu, Shenglong
    Wang, Fuhui
    APPLIED SURFACE SCIENCE, 2013, 268 : 103 - 110
  • [33] Na2SO4- and NaCl-induced hot corrosion behaviors of a nickel-base superalloy with aluminide diffusion coating
    An, TF
    Guan, HR
    Sun, XF
    Hu, ZQ
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2001, 16 (01): : 59 - 62
  • [35] Grain size dependant high-temperature hot corrosion (HTHC) degradation behavior in Alloy 617 during exposure in Na2SO4 + NaCl + V2O5 salt mixture
    Bhuyan, P.
    Sanyal, S.
    Mitra, R.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 914
  • [36] Hot corrosion behaviour of Inconel 738 superalloy in presence of NaCl, Na2SO4, V2O5
    Patil, Arpit R.
    Vagge, S. T.
    MATERIALS TODAY-PROCEEDINGS, 2022, 65 : 74 - 80
  • [37] Hot corrosion behavior and mechanism of FGH96 P/M superalloy in molten NaCl–Na2SO4 salts
    He Jiang
    Jian-Xin Dong
    Mai-Cang Zhang
    Lei Zheng
    Zhi-Hao Yao
    Rare Metals, 2019, 38 : 173 - 180
  • [38] Hot corrosion behavior and mechanism of FGH96 P/M superalloy in molten NaCl–Na2SO4 salts
    He Jiang
    Jian-Xin Dong
    Mai-Cang Zhang
    Lei Zheng
    Zhi-Hao Yao
    Rare Metals, 2019, 38 (02) : 173 - 180
  • [39] Hot Corrosion Behavior of Inconel625 Alloy and Welds in Na2SO4-NaCl Molten Salt
    Zhang Zhongke
    Xiong Jianqiang
    Chu Shusheng
    Li Xuanbai
    Jiang Changming
    RARE METAL MATERIALS AND ENGINEERING, 2023, 52 (05) : 1842 - 1850
  • [40] Hot corrosion behavior of Mg2SiO4 ceramic exposed to molten Na2SO4 at 900°C to 1100°C
    Milles, Hamza
    Snani, Louafi
    Oulabbas, Amel
    Toualbia, Khaled
    JOURNAL OF METALS MATERIALS AND MINERALS, 2024, 34 (01):