Hot Corrosion Behavior of Si-Y-Co-Modified Aluminide Coating Exposed to NaCl + Na2SO4 Salt at 1173 K

被引:11
|
作者
Liu, Zongjie [1 ]
Zhou, Chungen [1 ]
机构
[1] Beijing Univ Aeronaut & Astronaut, Sch Mat Sci & Engn, Key Lab Aerosp Mat & Performance, Minist Educ, Beijing 100191, Peoples R China
来源
OXIDATION OF METALS | 2016年 / 85卷 / 1-2期
基金
中国国家自然科学基金;
关键词
Metal coatings; Superalloys; Hot corrosion; CYCLIC OXIDATION BEHAVIOR; PHASE-TRANSFORMATIONS; SILICON; RESISTANCE; ALLOY; PACK; AL;
D O I
10.1007/s11085-015-9599-3
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The microstructure and hot corrosion behavior of a Si-Y-Co-modified aluminide coating prepared on a nickel base superalloy DZ125 by the pack cementation process was studied. The Co-Al-Si-Y coated specimen had a mass gain of only 0.25 mg/cm(2) after being exposed to NaCl + Na2SO4 salt for 100 h at 1173 K. Thus the addition of Si to a Y-Co-modified aluminide coating increased its hot corrosion resistance by 40 %. The improved hot corrosion resistance of the Co-Al-Si-Y coating was mainly attributed to the formation of an Al2O3 scale with SiO2 on the surface of the coating during the hot corrosion test. SiO2 can prohibit the high fluxing rate of dissolution of the protective Al2O3 scale and prevent rapid corrosion attack owing to its low solubility over a wide range of salt acidity and its weak oxygen permeability. Graphical Abstract The Co-Al-Si-Y coated specimen had a mass gain of only 0.25 mg/cm(2) after being exposed to NaCl + Na2SO4 salt for 100 h at 1173 K. The addition of Si to a Y-Co-modified aluminide coating improved its hot corrosion resistance. [GRAPHICS]
引用
收藏
页码:205 / 217
页数:13
相关论文
共 50 条
  • [21] Hot corrosion behavior of SiC in molten Na2SO4
    Nakagawa, T
    Hara, M
    Imai, K
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1997, 61 (11) : 1241 - 1248
  • [22] Comparison investigation of hot corrosion exposed to Na2SO4 salt and oxidation of MoSi2-based coating on Nb alloy at 1000 °C
    Sun, Le
    Fu, Qian-Gang
    Sun, Jia
    Zhang, Guang-peng
    SURFACE & COATINGS TECHNOLOGY, 2020, 385 (385)
  • [23] Hot corrosion behavior of a centimeter Fe-based amorphous composite coating prepared by laser cladding in molten Na2SO4 + K2SO4 salts
    Liu, Wenyi
    Hou, Yong
    Liu, Chao
    Wang, Yongtian
    Jiang, Runsen
    Xu, Gang
    SURFACE & COATINGS TECHNOLOGY, 2015, 270 : 33 - 38
  • [24] Hot Corrosion Behavior of ZrB2-SiC-Graphite Composite in NaCl and Na2SO4 Molten Salts
    Liu, X.
    Wang, G.
    Liu, L.
    Wang, Z.
    Wu, Z.
    Liu, M.
    JOURNAL OF CERAMIC SCIENCE AND TECHNOLOGY, 2018, 9 (03): : 309 - 317
  • [25] Hot corrosion behavior of a Si-Y co-deposition coating on a Ti2AlNb based alloy in NaCl-Na2SO4 mixture
    Xiang, Jiayi
    Xie, Faqin
    Wu, Xiangqing
    Wang, Shaoqing
    Li, Lang
    SURFACE & COATINGS TECHNOLOGY, 2021, 419
  • [26] Effect of Minor Nb on Isothermal-Oxidation and Hot Corrosion Behavior of Two Nickel-Based Superalloys Under Na2SO4/Na2SO4-NaCl
    Zhou, Yuebo
    Wang, Hong
    Mo, Chenggang
    Zhang, Lina
    CORROSION, 2021, 77 (09) : 949 - 960
  • [27] Hot Corrosion Behavior of Ce-Modified NiAl Coating by Cl-Containing Na2SO4 at 1050 °C
    Hongyu Wang
    Han Wang
    Peng Kan
    Qian Zhao
    Xiang Zhang
    Yang Ding
    Oxidation of Metals, 2018, 90 : 571 - 583
  • [28] Hot Corrosion Behavior of Inconel 625 in Na2SO4 and V2O5 Molten Salt System
    Li, Liang
    Li, Lanfeng
    Zhang, Guofeng
    Xue, Hongdi
    Cui, Maomao
    Wang, Wenxu
    Liu, Dexue
    METALS, 2023, 13 (06)
  • [29] Hot corrosion behaviour of Nbss/Nb5Si3 in situ composites in the mixture of Na2SO4 and NaCl melts
    Wang, Wan
    Zhou, Chungen
    CORROSION SCIENCE, 2013, 74 : 345 - 352
  • [30] Effects of Pt and Si on the low temperature hot corrosion of aluminide coatings exposed to Na2SO4-60 mol% V2O5 salt
    Azarmehr, S. A.
    Shirvani, K.
    Solimani, A.
    Schuetze, M.
    Galetz, M. C.
    SURFACE & COATINGS TECHNOLOGY, 2019, 362 : 252 - 261