Hydride Reorientation and Delayed Hydride Cracking of Spent Fuel Rods in Dry Storage

被引:4
作者
Kim, Young S. [1 ]
机构
[1] Korea Atom Energy Res Inst, Nucl Mat Res Div, Taejon 305353, South Korea
来源
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 2009年 / 40A卷 / 12期
关键词
PRESSURE TUBE MATERIAL; ZIRCONIUM ALLOYS; TERMINAL SOLUBILITY; HYDROGEN; PRECIPITATION; TEMPERATURE; STRESS; DISSOLUTION; OXIDATION; BEHAVIOR;
D O I
10.1007/s11661-009-0044-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The aim of this work is to investigate the effect of thermal creep during vacuum drying of spent fuel rods on hydride reorientation and their delayed hydride cracking (DHC) susceptibility. To these ends, we analyzed Tsai's thermal creep results of irradiated Zircaloy-4 cladding segments from two pressurized water reactors and Simpson and Ells' observation where zirconium alloy cladding tube failed during long-term storage at room temperature. On cooling under 190 MPa, the spent fuel rods crept to 3.5 pct strain during vacuum drying showed large radial hydrides, while the ones crept to 0.35 pct strain had very fine radial hydrides. Thus, it is suggested that prior creep deformation promotes hydride reorientation in spent fuel rods on cooling after vacuum drying. Evidence for this suggestion is provided by a model experiment. Considering Kim's DHC model and experimental facts showing precipitation of hydrides even at room temperature at stress raisers, we suggest that spent fuel rods would fail by DHC in dry storage if stress raisers are present inside the cladding on cooling to below 180 degrees C, and then axial splits of the failed spent fuel rods would occur by DHC due to fuel expansion by UO2 oxidation.
引用
收藏
页码:2867 / 2875
页数:9
相关论文
共 38 条
[31]   EFFECTS OF CRACK TIP STRESS STATES AND HYDRIDE-MATRIX INTERACTION STRESSES ON DELAYED HYDRIDE CRACKING [J].
PULS, MP .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1990, 21 (11) :2905-2917
[32]   Neutron diffraction study of the precipitation and dissolution of hydrides in Zr-2.5Nb pressure tube material [J].
Root, JH ;
Fong, RWL .
JOURNAL OF NUCLEAR MATERIALS, 1996, 232 (01) :75-85
[33]   HYDROGEN CONCENTRATION LIMIT AND CRITICAL-TEMPERATURES FOR DELAYED HYDRIDE CRACKING IN ZIRCONIUM ALLOYS [J].
SHI, SQ ;
SHEK, GK ;
PULS, MP .
JOURNAL OF NUCLEAR MATERIALS, 1995, 218 (02) :189-201
[34]   DELAYED HYDROGEN EMBRITTLEMENT IN ZR-2.5 WT PERCENT NB [J].
SIMPSON, CJ ;
ELLS, CE .
JOURNAL OF NUCLEAR MATERIALS, 1974, 52 (02) :289-295
[35]  
Simpson L.A., 1977, ASTM Spec. Tech. Publ., V633, P608
[36]  
TSAI H, 2006, J ASTM INT, V3, P632
[37]  
YANG RL, 2004, P 2004 INT M LWR FUE, P565
[38]  
YUN YB, 2003, J KOR NUCL SOC, V35, P529