Ytterbium disilicate-based glass-ceramic as joining material for ceramic matrix composites

被引:20
|
作者
Smeacetto, Federico [1 ]
D'Isanto, Fabiana [1 ]
Casalegno, Valentina [1 ]
Tatarko, Peter [2 ]
Salvo, Milena [1 ]
机构
[1] Politecn Torino, DISAT, Dept Appl Sci & Technol, Corso Duca Abruzzi 24, I-10129 Turin, Italy
[2] Slovak Acad Sci, Inst Inorgan Chem, Dubravska Cesta 9, Bratislava 84536, Slovakia
关键词
Joining; Glass; Ceramic matrix composites; INTERLAYER;
D O I
10.1016/j.jeurceramsoc.2020.10.022
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A key aspect of ceramic matrix composites integration is related to a reliable joining technique. An ytterbium disilicate based glass-ceramic material is processed by reactive viscous flow sintering between a barium aluminium borosilicate glass and ytterbium oxide and it is used to join SiC/SiC and C/SiC composites. The joining temperature and the in situ formation of the Yb2Si2O7 is optimised at 1200 degrees C without pressure, on the basis of the sintering and crystallisation mechanisms. The mechanical characterization of SiC/SiC and C/SiC joined with the ytterbium disilicate-based glass-ceramic, tested by single-lap offset at RT, exhibits an apparent shear strength of 35 MPa, similar to their interlaminar shear strength. The proposed system displays self-healing behaviour at 1000 degrees C and 1150 degrees C, as demonstrated by the partial and complete sealing of induced cracks by Vickers indentation on its surface at different loads, thus suggesting that it can effectively be used as promising joining material for CMCs.
引用
收藏
页码:1099 / 1106
页数:8
相关论文
共 50 条
  • [31] Microstructure and mechanical properties of zirconia-toughened lithium disilicate glass-ceramic composites
    Huang, X.
    Zheng, X.
    Zhao, G.
    Zhong, B.
    Zhang, X.
    Wen, G.
    MATERIALS CHEMISTRY AND PHYSICS, 2014, 143 (02) : 845 - 852
  • [32] Glass as a joining material for ceramic matrix composites: 25 years of research at Politecnico di Torino
    Ferraris, Monica
    Casalegno, Valentina
    Smeacetto, Federico
    Salvo, Milena
    INTERNATIONAL JOURNAL OF APPLIED GLASS SCIENCE, 2020, 11 (03) : 569 - 576
  • [33] JOINING OF CERAMIC-MATRIX COMPOSITES
    CAWLEY, JD
    AMERICAN CERAMIC SOCIETY BULLETIN, 1989, 68 (09): : 1619 - 1623
  • [34] Glass and glass-ceramic matrix composite materials
    Boccaccini, AR
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2001, 109 (07) : S99 - S109
  • [35] Creep of some glass-ceramic composites
    Chermant, JL
    Doreau, F
    Maupas, H
    Vicens, J
    CREEP AND FRACTURE OF ENGINEERING MATERIALS AND STRUCTURES, 1996, : 601 - 610
  • [36] METALLIC-GLASS RIBBON-REINFORCED GLASS-CERAMIC MATRIX COMPOSITES
    VAIDYA, RU
    SUBRAMANIAN, KN
    JOURNAL OF MATERIALS SCIENCE, 1990, 25 (07) : 3291 - 3296
  • [37] Glass and glass-ceramic matrix composites: from model systems to useful materials
    Boccaccini, AR
    Kaya, C
    ADVANCED FIBERS, PLASTICS, LAMINATES AND COMPOSITES, 2002, 702 : 277 - 288
  • [38] Hi NicalonTM SiC fiber reinforced glass and glass-ceramic matrix composites
    United Technologies Research Cent, East Hartford, United States
    Ceram Eng Sci Proc, 4 (291-298):
  • [39] Influence of the reactivity of inorganic fillers to a glass matrix on the properties of glass-ceramic composites
    Mizutani, H
    Sato, M
    Yokoi, H
    Ohbayashi, K
    Iio, S
    DIELECTRIC CERAMIC MATERIALS, 1999, 100 : 277 - 286
  • [40] TOUGHENING IN METALLIC-GLASS RIBBON REINFORCED GLASS-CERAMIC MATRIX COMPOSITES
    VAIDYA, RU
    SUBRAMANIAN, KN
    SAMPE JOURNAL, 1993, 29 (04) : 26 - 30