摘要
This study reports an example of visible-light photocatalyst based on TiO2 modified by ruthenium-complex sensitizers and noble metal deposits. The photodegradation of trichloroacetate (TCA) and carbon tetrachloride was used as a probe reaction for evaluating the visible light activity of the photocatalyst under the illumination of lambda > 420 nm. Photodeposition of platinum nanoparticles on dye-sensitized TiO2 (Pt/TiO2/(RuL3)-L-II) drastically enhanced the degradation rate of TCA and CCl4. The visible light reactivity of Pt/TiO2/(RuL3)-L-II was optimal with [(RuL3)-L-II] = 10 muM, [TiO2] = 0.5 g/L, and Pt loading of about 0.2 wt %. Although no electron donors to regenerate the oxidized Ru-sensitizers were added in the aqueous suspension, the photoreductive dechlorination of perchlorinated compounds proceeded far beyond the stoichiometric limit of the initial sensitizer concentration. Water acted as an electron donor to regenerate the sensitizer with a concurrent production of dioxygen. On the other hand, Pt/TiO2/(RuL3)-L-II was completely inactive in the presence of dissolved oxygen and the in-situ generated dioxygen gradually decelerated the dechlorination rate. Conduction band electrons transferred to 02 in preference to CCl4 and TCA on Pt deposits. Other noble metals (Ag, Au, and Pd) deposited on TiO2 showed a better oxygen-tolerance but less visible-light reactivity than Pt/TiO2/(RuL3)-L-II. Effects of metal loading on the visible light activity and its implications for the efficient visible-light photocatalyst development are discussed.
引用
收藏
页码:147 / 152
页数:6
相关论文
共 41 条
[1]   Steady hydrogen evolution from water on Eosin Y-fixed TiO2 photocatalyst using a silane-coupling reagent under visible light irradiation [J].
Abe, R ;
Hara, K ;
Sayama, K ;
Domen, K ;
Arakawa, H .
JOURNAL OF PHOTOCHEMISTRY AND PHOTOBIOLOGY A-CHEMISTRY, 2000, 137 (01) :63-69
[2]   Visible-light photocatalysis in nitrogen-doped titanium oxides [J].
Asahi, R ;
Morikawa, T ;
Ohwaki, T ;
Aoki, K ;
Taga, Y .
SCIENCE, 2001, 293 (5528) :269-271
[3]   EFFICIENT PHOTOCATALYSIS OF THE IRREVERSIBLE ONE-ELECTRON AND 2-ELECTRON REDUCTION OF HALOTHANE ON PLATINIZED COLLOIDAL TITANIUM-DIOXIDE IN AQUEOUS SUSPENSION [J].
BAHNEMANN, DW ;
MONIG, J ;
CHAPMAN, R .
JOURNAL OF PHYSICAL CHEMISTRY, 1987, 91 (14) :3782-3788
[4]   A STUDY OF THE PRIMARY STEP IN THE PHOTOCHEMICAL DEGRADATION OF ACETIC-ACID AND CHLOROACETIC ACIDS ON A TIO2 PHOTOCATALYST [J].
CHEMSEDDINE, A ;
BOEHM, HP .
JOURNAL OF MOLECULAR CATALYSIS, 1990, 60 (03) :295-311
[5]   Visible light-induced degradation of carbon tetrachloride on dye-sensitized TiO2 [J].
Cho, YM ;
Choi, WY ;
Lee, CH ;
Hyeon, T ;
Lee, HI .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2001, 35 (05) :966-970
[6]   Investigation on TiO2-coated optical fibers for gas-phase photocatalytic oxidation of acetone [J].
Choi, W ;
Ko, JY ;
Park, H ;
Chung, JS .
APPLIED CATALYSIS B-ENVIRONMENTAL, 2001, 31 (03) :209-220
[7]   Photocatalytic degradation of polychlorinated dibenzo-p-dioxins on TiO2 film under UV or solar light irradiation [J].
Choi, W ;
Hong, SJ ;
Chang, YS ;
Cho, Y .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2000, 34 (22) :4810-4815
[8]   THE ROLE OF METAL-ION DOPANTS IN QUANTUM-SIZED TIO2 - CORRELATION BETWEEN PHOTOREACTIVITY AND CHARGE-CARRIER RECOMBINATION DYNAMICS [J].
CHOI, WY ;
TERMIN, A ;
HOFFMANN, MR .
JOURNAL OF PHYSICAL CHEMISTRY, 1994, 98 (51) :13669-13679
[9]   Kinetics and mechanism of CCl4 photoreductive degradation on TiO2: The role of trichloromethyl radical and dichlorocarbene [J].
Choi, WY ;
Hoffmann, MR .
JOURNAL OF PHYSICAL CHEMISTRY, 1996, 100 (06) :2161-2169
[10]   Novel photocatalytic mechanisms for CHCl3, CHBr3, and CCl3CO2- degradation and the fate of photogenerated trihalomethyl radicals on TiO2 [J].
Choi, WY ;
Hoffmann, MR .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 1997, 31 (01) :89-95