A Small-Scale Test to Examine Heat Delamination in Cross Laminated Timber (CLT)

被引:10
作者
Miyamoto, Byrne [1 ]
Bechle, Nathan J. [2 ]
Rammer, Douglas R. [2 ]
Zelinka, Samuel L. [2 ]
机构
[1] Oregon State Univ, Tallwood Design Inst, Corvallis Oregon, OR 97331 USA
[2] US Forest Serv, USDA, Forest Prod Lab, Madison, WI 53726 USA
基金
美国国家科学基金会;
关键词
mass timber; cross laminated timber (CLT); fire performance; fire regrowth; delamination; creep tests;
D O I
10.3390/f12020232
中图分类号
S7 [林业];
学科分类号
0829 ; 0907 ;
摘要
This paper examines the strength of wood adhesive bonds at high temperatures. The goal of this research is to better understand the conditions of heat delamination in cross laminated timber (CLT) that is exposed to fire. Heat delamination in CLT occurs when one lamination detaches from the composite panel before the char front reaches the bondline. Timber that falls from the panel, as a result of delamination, contributes additional fuel to the fire, which can cause fire regrowth, while the loss of a lamination causes a sudden loss in strength. Currently, to demonstrate that an adhesive does not delaminate, it must pass a full scale (6 m by 3 m) compartment fire test as prescribed in the PRG-320 product standard. In this work, we scaled down the mechanical loads and temperatures to 300 mm lap shear specimens. Seven different adhesives were tested and compared against solid wood controls with the same geometry as the lap shear specimens. Quasi-static tests were run where the specimens were loaded to failure at 25 degrees C and 260 degrees C, when the samples were at thermal equilibrium. Additionally, creep tests were performed where the load and temperature ramp was matched to the adhesive bondline temperatures measured in the large scale PRG-320 tests. With the exception of some of the polyurethane formulations, all adhesives passed the scaled-down creep test that resembles the PRG-320 standard. Of the polyurethane adhesives tested, only one formulation remained intact for the duration of the test. These results can be used to help better predict which adhesives may pass the PRG-320 test prior to full scale testing.
引用
收藏
页码:1 / 11
页数:11
相关论文
共 24 条
[1]  
[Anonymous], 2016, ASTM D6815 09 AM SOC
[2]  
[Anonymous], 2021, International Building Code
[3]  
[Anonymous], 2018, ANSI/APA PRG 320-Standard for Performance-Rated Cross Laminated Timber
[4]  
Fitz-Thedmar A., 1274, LIBER ANTIQUS LEGIBU
[5]  
Gerard Robert., 2013, FIRE SAFETY CHALLENG
[6]  
Hasburgh L.E., 2018, P WORLD C TIMB ENG S
[7]  
Iqbal A., 2018, 1 INT C NEW HOR GREE, P111
[8]  
Janssens M., 2017, MASS PLYWOOD PANEL E
[9]  
Janssens M., 2017, SwRI Project No.01.23086.01.001a
[10]  
Karsh J., 2012, Report prepared for the Canadian wood council on behalf of the wood enterprise coalition and forest innovation investment