Fracture toughness anisotropy of Ti17 billet processed by the β forging

被引:23
作者
Chen, Wei [1 ,2 ,3 ]
Zeng, Weidong [1 ,2 ,3 ]
Zhao, Yaohua [1 ,2 ,3 ]
Gao, Pan [1 ,2 ,3 ]
Xu, Jianwei [1 ,2 ,3 ]
Zhao, Qinyang [4 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Sch Mat Sci & Engn, Xian 710072, Peoples R China
[2] Northwestern Polytech Univ, Def Technoloies Innovat Ctr Precis Forging & Ring, Sch Mat Sci & Engn, Xian 710072, Peoples R China
[3] Northwestern Polytech Univ, Shaanxi Key Lab High Performance Precis Forming T, Xian 710072, Peoples R China
[4] Changan Univ, Sch Mat Sci & Engn, Xian 710064, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2021年 / 807卷
基金
中国博士后科学基金;
关键词
Titanium alloy; β forging; Fracture toughness; Anisotropy; Delamination;
D O I
10.1016/j.msea.2021.140825
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The fracture behavior of Ti17 billet processed by the beta forging was examined. The results demonstrate that the specimen orientation has a pronounce effect on the fracture toughness value as well as on the crack propagation path. The fracture anisotropy can be attributed to the elongated and aligned beta grain. The crack preferentially nucleates and propagates along the precipitate-free zone nearby the grain boundary. It causes either crack deflection or delamination, enhancing the fracture resistance as compared to one weak specimen orientation. The exceptionally good combination of strength and fracture toughness can be achieved by activating delamination toughening. The delamination transforms the fracture under plane-strain condition into a series of fracture processes in plane-stress condition through the thickness, and the fracture toughness is enhanced. Furthermore, a fracture toughness prediction model considering both the intrinsic and extrinsic contributions is constructed. The results show that the extrinsic toughness varies greatly than the intrinsic toughness in different orientations, indicating that the extrinsic toughness plays a significant role in the fracture toughness anisotropy of the Ti17 billet.
引用
收藏
页数:12
相关论文
共 46 条
[1]  
Anderson T.L., 1991, FRACTURE MECH
[2]   Optimal design of aircraft structures with damage tolerance requirements [J].
Arrieta, AJ ;
Striz, AG .
STRUCTURAL AND MULTIDISCIPLINARY OPTIMIZATION, 2005, 30 (02) :155-163
[3]   Perspectives on Titanium Science and Technology [J].
Banerjee, Dipankar ;
Williams, J. C. .
ACTA MATERIALIA, 2013, 61 (03) :844-879
[4]   An overview on the use of titanium in the aerospace industry [J].
Boyer, RR .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 213 (1-2) :103-114
[5]   SLIGHTLY CURVED OR KINKED CRACKS [J].
COTTERELL, B ;
RICE, JR .
INTERNATIONAL JOURNAL OF FRACTURE, 1980, 16 (02) :155-169
[6]   Microstructural morphology effects on fracture resistance and crack tip strain distribution in Ti-6Al-4V alloy for orthopedic implants [J].
Cvijovic-Alagic, I. ;
Gubeljak, N. ;
Rakin, M. ;
Cvijovic, Z. ;
Geric, K. .
MATERIALS & DESIGN, 2014, 53 :870-880
[7]   Improving the ductility of nanocrystalline bcc metals [J].
Farkas, D ;
Hyde, B .
NANO LETTERS, 2005, 5 (12) :2403-2407
[8]   Simulations of intergranular fracture in nanocrystalline molybdenum [J].
Frederiksen, SL ;
Jacobsen, KW ;
Schiotz, J .
ACTA MATERIALIA, 2004, 52 (17) :5019-5029
[9]   Microstructure-fracture toughness correlation in an aircraft structural component alloy Ti-5Al-5V-5Mo-3Cr [J].
Ghosh, Atasi ;
Sivaprasad, S. ;
Bhattacharjee, Amit ;
Kar, Sujoy Kumar .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 568 :61-67
[10]   RECRYSTALLIZATION AND SUPERPLASTICITY AT 300-DEGREES-C IN AN ALUMINUM-MAGNESIUM ALLOY [J].
HALES, SJ ;
MCNELLEY, TR ;
MCQUEEN, HJ .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1991, 22 (05) :1037-1047