Tensile strength of thermally modified laminated strand lumber and laminated veneer lumber

被引:11
作者
Aro, Matthew D. [1 ]
Wang, Xiping [2 ]
McDonald, Dwight E. [2 ]
Begel, Marshall [2 ]
机构
[1] Nat Resources Res Inst, 5013 Miller Trunk Highway, Duluth, MN 55811 USA
[2] US Forest Serv, USDA, Forest Prod Lab, Madison, WI USA
基金
美国国家科学基金会;
关键词
Engineered wood; modified wood; thermally modified wood; MECHANICAL-PROPERTIES; CHEMICAL-COMPOSITION; HEAT-TREATMENT; WOOD; BIRCH;
D O I
10.1080/17480272.2016.1164246
中图分类号
TB3 [工程材料学]; TS [轻工业、手工业、生活服务业];
学科分类号
0805 ; 080502 ; 0822 ;
摘要
Laminated strand lumber (LSL) and laminated veneer lumber (LVL) were thermally modified as a post-treatment at 140 degrees C, 150 degrees C, 160 degrees C, 170 degrees C, and 180 degrees C. The tension modulus of elasticity (MOE) of LSL was not significantly impacted by the treatments, with the 180 degrees C treatment group exhibiting the highest tension MOE (11.8GPa). The LVL also experienced minimal impacts, with the 150 degrees C treatment group having the highest tension MOE (19.4GPa) and the 160 degrees C treatment group exhibiting the lowest (17.1GPa). The maximum tensile strength (MTS) of the LSL and LVL significantly decreased with increasing temperatures, with the control and 180 degrees C treatment groups experiencing the highest and lowest MTS, respectively. The lowest MTS for LSL was 10.8MPa (180 degrees C treatment), which was 70% lower than the controls. The lowest MTS of the LVL was 24.4MPa (also at the 180 degrees C treatment), which was a 49% decrease compared to the controls. These results suggest that thermal-modification post-treatments minimally impact tension MOE, but can significantly reduce MTS at higher treatment temperatures. Combined with previous work improving the moisture properties and equilibrium moisture content of thermally modified LSL and LVL, it may be possible to optimize the treatment technique(s) to yield products with desirable properties.
引用
收藏
页码:228 / 235
页数:8
相关论文
共 40 条
  • [1] [Anonymous], 2013, ANN BOOK ASTM STAND, V15.06
  • [2] [Anonymous], 2007, ANN BOOK ASTM STAND
  • [3] [Anonymous], 1984, WOOD CHEM ULTRASTRUC, DOI DOI 10.1515/9783110839654
  • [4] [Anonymous], SPEC SEM 9 FEBR 2001
  • [5] Mechanical and Physical Properties of Thermally Modified Plywood and Oriented Strand Board Panels
    Aro, Matthew D.
    Brashaw, Brian K.
    Donahue, Patrick K.
    [J]. FOREST PRODUCTS JOURNAL, 2014, 64 (7-8) : 281 - 289
  • [6] Concomitant Changes in Viscoelastic Properties and Amorphous Polymers during the Hydrothermal Treatment of Hardwood and Softwood
    Assor, Carole
    Placet, Vincent
    Chabbert, Brigitte
    Habrant, Anouck
    Lapierre, Catherine
    Pollet, Brigitte
    Perre, Patrick
    [J]. JOURNAL OF AGRICULTURAL AND FOOD CHEMISTRY, 2009, 57 (15) : 6830 - 6837
  • [7] Bodig J., 1982, MECH WOOD WOOD COMPO
  • [8] Bonigut J., 2012, 6 EUR C WOOD MOD P S, P175
  • [9] Thermal modification of consolidated oriented strandboards: effects on dimensional stability, mechanical properties, chemical composition and surface color
    Del Menezzi, C. H. S.
    Tomaselli, I.
    Okino, E. Y. A.
    Teixeira, D. E.
    Santana, M. A. E.
    [J]. EUROPEAN JOURNAL OF WOOD AND WOOD PRODUCTS, 2009, 67 (04) : 383 - 396
  • [10] Donahue P., 2011, 09DG090 USDA WOOD ED