Controlling the textural parameters of mesoporous carbon materials
被引:112
作者:
Vinu, A.
Srinivasu, P.
Takahashi, M.
Mori, T.
Balasubramanian, V. V.
Ariga, K.
机构:
[1] Natl Inst Mat Sci, Fuel Cell Mat Ctr, Nanoion Mat Grp, Tsukuba, Ibaraki 3050044, Japan
[2] Soonchunhyang Univ, Dept Marine Biotechnol, Asan 336745, Chungnam, South Korea
[3] Natl Inst Mat Sci, Adv Mat Lab, Supermol Grp, Tsukuba, Ibaraki 3050044, Japan
关键词:
mesoporous carbon;
molecular sieves;
adsorption;
surface properties;
CMK-3;
D O I:
10.1016/j.micromeso.2006.10.008
中图分类号:
O69 [应用化学];
学科分类号:
081704 ;
摘要:
The mesoporous carbon materials prepared by inorganic templating technique using mesoporous silica, SBA-15 as a template and sucrose as a carbon source, have been systematically investigated as a function of sucrose to mesoporous silica composition, with a special focus on controlling the mesoporous structure, surface morphology and the textural parameters such as specific surface area, specific pore volume and pore size distribution. All the materials have been unambiguously characterized by XRD, N-2 adsorption-desorption isotherms, high-resolution transmission electron microscopy, high-resolution field emission scanning electron microscopy, and Raman spectroscopy. It has been found that the porous structure, morphology and the textural parameters of the mesoporous carbons materials, CMK-3-x where x represent the sucrose to silica weight ratio, can be easily controlled by the simple adjustment of concentration of sucrose molecules. It has also been found that the specific surface area of the mesoporous carbon materials systematically increases with decreasing the sucrose to silica weight ratio. Moreover, the specific pore volume of the materials increases from 0.57 to 1.31 cm(3)/g with decreasing the sucrose to silica weight ratio from 5 to 1.25 and then decreases to 1.23 cm(3)/g for CMK-3-0.8. HRTEM and HR-FESEM also show a highly ordered pore structure and better surface morphology for CMK-3-1.25 as compared to other materials prepared in this study. Thus, it can be concluded that the sucrose to silica weight ratio of 1.25 is the best condition to prepare well ordered mesoporous carbon materials with good textural parameters, pore structure and narrow pore size distribution. (c) 2006 Elsevier Inc. All rights reserved.