Cushioning energy absorption of paper corrugation tubes with regular polygonal cross-section under axial static compression

被引:4
作者
Kang, Jianfen [1 ]
Guo, Yanfeng [1 ]
Fu, Yungang [1 ]
Li, Qiong [1 ]
Lv, Yabo [1 ]
机构
[1] Xian Univ Technol, Fac Printing Packaging Engn & Digital Media Techn, Xian 710048, Shaanxi, Peoples R China
基金
中国国家自然科学基金;
关键词
paper corrugation tube; axial static compression; folding model; deformation mode; cushioning energy absorption; mean crush force; BEHAVIOR; CORE;
D O I
10.1515/secm-2021-0003
中图分类号
TB33 [复合材料];
学科分类号
摘要
The paper corrugation tube is an innovative kind of energy absorbing structure and shock absorber which can play an important role on the cushioning energy absorption for airdrop equipments and transportation packaging. The deformation characteristics and failure modes of the regular triangle, quadrangle, pentagon and hexagon paper corrugation tubes were comparatively studied by a series of axial static compression experiments, the cushioning energy absorption was evaluated by the seven characteristic parameters (e.g. initial peak force, mean crush force, total energy absorption, specific energy absorption, crush force efficiency, unit area energy absorption and stroke efficiency), and the influences of tube direction, cross-sectional shape, tube length and compression rate on failure modes and cushioning energy absorption were analyzed and compared. These researches showed that the tubes along X direction only have the accordion deformation mode, yet the tubes along Y direction have four deformation modes including steady state progressive buckling, Euler buckling, angular tear and transverse shear. For the paper corrugation tubes along Y direction, the cross-sectional shape has obvious influence on the cushioning energy absorption of structures, and the specific energy absorption and unit area energy absorption of regular triangle and pentagon tubes are better than those of the tubes with regular quadrilateral and hexagonal cross-section at compression rates of 12 and 48mm/min. The tube length of 150 mm or compression rate of 72 mm/min would cause the increase of contribution proportion of non-ideal deformation mode and the decrease of cushioning properties. The paper corrugation tubes along X direction have more stable and controllable deformation mode, yet the paper corrugation tubes along Y direction have better cushioning energy absorption.
引用
收藏
页码:24 / 38
页数:15
相关论文
共 23 条
[1]   Axial crushing behavior and energy absorption efficiency of corrugated tubes [J].
Eyvazian, Arameh ;
Habibi, Meisam K. ;
Hamouda, Abdel Magid ;
Hedayati, Reza .
MATERIALS & DESIGN, 2014, 54 :1028-1038
[2]  
Gao D, 2001, J VIBRATION ENG, V14, P172
[3]  
Guo YF, 2011, SHOCK VIB, V18, P525, DOI [10.3233/SAV-2010-0559, 10.1155/2011/578265]
[4]  
Guo YF, 2014, P 2 INT C PACK TECHN
[5]   Refined nonlinear finite element models for corrugated fiberboards [J].
Haj-Ali, Rami ;
Choi, Joonho ;
Wei, Bo-Siou ;
Popil, Roman ;
Schaepe, Michael .
COMPOSITE STRUCTURES, 2009, 87 (04) :321-333
[6]  
Hohe J., 2002, APPL MECH REV, V55, P61, DOI [DOI 10.1115/1.1425394, 10.1115/1.1425394]
[7]   Corrugated all-composite sandwich structures. Part 2: Failure mechanisms and experimental programme [J].
Kazemahvazi, Sohrab ;
Tanner, Daniel ;
Zenkert, Dan .
COMPOSITES SCIENCE AND TECHNOLOGY, 2009, 69 (7-8) :920-925
[8]   Numerical crushing analysis of aluminum foam-filled corrugated single- and double-circular tubes subjected to axial impact loading [J].
Kilicaslan, Cenk .
THIN-WALLED STRUCTURES, 2015, 96 :82-94
[9]   The impact responses and the finite element modeling of layered trapezoidal corrugated aluminum core and aluminum sheet interlayer sandwich structures [J].
Kilicaslan, Cenk ;
Guden, Mustafa ;
Odaci, Ismet Kutlay ;
Tasdemirci, Alper .
MATERIALS & DESIGN, 2013, 46 :121-133
[10]   Hierarchical corrugated core sandwich panel concepts [J].
Kooistra, Gregory W. ;
Deshpande, Vikram ;
Wadley, Haydn N. G. .
JOURNAL OF APPLIED MECHANICS-TRANSACTIONS OF THE ASME, 2007, 74 (02) :259-268