The effect of test temperature on SCC behavior of austenitic stainless steels in boiling saturated magnesium chloride solution

被引:51
|
作者
Alyousif, Osama M.
Nishimura, Rokuro
机构
[1] Osaka Prefecture Univ, Coll Engn, Dept Appl Mat Sci, Sakai, Osaka, Japan
[2] Kuwait Univ, Dept Engn Mech, Safat 13060, Kuwait
关键词
austenitic stainless steels; magnesium chloride solutions; steady-state elongation rates; stress corrosion cracking; hydrogen embrittlement;
D O I
10.1016/j.corsci.2006.01.014
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The stress corrosion cracking (SCC) of the austenitic stainless steels of types 304, 310 and 316 was investigated as a function of test temperature in boiling saturated magnesium chloride solution (MgCl2) using a constant load method. Both of types 304 and 316 exhibited similar corrosion elongation curves, while the corrosion elongation curve of type 310 was different from those of types 304 and 316, in terms of the three parameters such as time to failure (t(f)), steady-state elongation rate (l(ss)) and transition time to time to failure ratio (t(ss)/t(f)) obtained from the corrosion elongation curves for these stainless steels. The relationship between the time to failure and a reciprocal cf test temperature fell in two straight lines on a semi-logarithmic scale as well as the relationship between the steadystate elongation rate and a reciprocal of test temperature. These regions were considered to correspond to a SCC-dominated region and a hydrogen embrittlement (HE)-dominated region from the value of (t(ss)/t(f)) and the fracture appearance. The relationship between the steady state elongation rates versus time to failure on a logarithmic scale became a straight line, whereas the slopes of the line for the stainless steels were different with the different fracture mechanism iuch as SCC and HE. It was found that the linearity of the relationship can be used to predict the time to failure for the stainless steels in the corrosive environment. In addition, type 310 did not suffer from HE, which means that type 310 showed only SCC. This would be explained by whether or not a formation of alpha'-martensite takes place. (c) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:4283 / 4293
页数:11
相关论文
共 46 条
  • [31] Influence of temperature and stress state on the TWIP behavior of 201LN and 316LV austenitic stainless steels
    Braga, Diogo Pedrino
    Corre, Leonardo Muthi
    Sordi, Vitor Luiz
    Rovere, Carlos Alberto Della
    Cintho, Osvaldo Mitsuyuki
    Kliauga, Andrea Madeira
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 863
  • [32] Comparative study on the effect of hydrogen charging on the passivity behavior of super stainless steels under acidic environment: Super duplex vs. super austenitic stainless steels
    Pedanekar, Rupesh S.
    Jamadar, Aasiya S.
    Park, Jin Sung
    Kim, Sung Jin
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2025, 116 : 516 - 529
  • [33] Effect of surface nanocrystallization induced by mechanical grinding treatment on stress corrosion cracking behavior of 316 L austenitic stainless steel in boiling MgCl2 solution
    Yang, Chongwen
    Jiang, Xinli
    Zhang, Wenqian
    Wang, Xuelin
    MATERIALS CHARACTERIZATION, 2024, 218
  • [34] Effect of Nb/Ti/Zr/W on precipitation behavior and mechanical property of 310S austenitic stainless steels
    Wen Dong-hui
    Lyu Yang
    Li Zhen
    Wang Qing
    Tang Rui
    Dong Chuang
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2019, 47 (09): : 61 - 71
  • [35] Distinguishing effect of buffing vs. grinding, milling and turning operations on the chloride induced SCC susceptibility of 304L austenitic stainless steel
    Kumar, Pandu Sunil
    Acharyya, Swati Ghosh
    Rao, S. V. Ramana
    Kapoor, Komal
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 687 : 193 - 199
  • [36] Effect of Temperature on Internal Reversible Hydrogen Embrittlement of SUH660 Iron-Based Superalloy and Austenitic Stainless Steels at Low Temperature
    Imade, Masaaki
    Zhang, Lin
    Iijima, Tadashi
    Fukuyama, Seiji
    Yokogawa, Kiyoshi
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2009, 73 (04) : 245 - 250
  • [37] The effect of sensitizing temperature on stress corrosion cracking of type 316 austenitic stainless steel in hydrochloric acid solution
    Nishimura, R
    Musalam, L
    Maeda, Y
    CORROSION SCIENCE, 2002, 44 (06) : 1343 - 1360
  • [38] The beneficial effect of surface carbon coating on stress corrosion cracking of Type 304 austenitic stainless steels in high temperature water
    Mukahiwa, K.
    Bertali, G.
    Burke, M. G.
    Duff, J.
    Scenini, F.
    SCRIPTA MATERIALIA, 2019, 158 : 77 - 82
  • [39] Effects of temperature and pressure on stress corrosion cracking behavior of 310S stainless steel in chloride solution
    Zhong, Yunpan
    Zhou, Cheng
    Chen, Songying
    Wang, Ruiyan
    CHINESE JOURNAL OF MECHANICAL ENGINEERING, 2017, 30 (01) : 200 - 206
  • [40] EFFECT OF POTENTIAL ON INTERACTION BETWEEN STRESS CORROSION CRACKING AND CORROSION FATIGUE OF AUSTENITIC STAINLESS STEEL IN BOILING 42% MgCl2 SOLUTION
    FENG Tao CHEN Liangshi KE Wei Corrosion Science Laboratory
    Acta Metallurgica Sinica(English Edition), 1991, (09) : 168 - 173