The effect of test temperature on SCC behavior of austenitic stainless steels in boiling saturated magnesium chloride solution

被引:51
|
作者
Alyousif, Osama M.
Nishimura, Rokuro
机构
[1] Osaka Prefecture Univ, Coll Engn, Dept Appl Mat Sci, Sakai, Osaka, Japan
[2] Kuwait Univ, Dept Engn Mech, Safat 13060, Kuwait
关键词
austenitic stainless steels; magnesium chloride solutions; steady-state elongation rates; stress corrosion cracking; hydrogen embrittlement;
D O I
10.1016/j.corsci.2006.01.014
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The stress corrosion cracking (SCC) of the austenitic stainless steels of types 304, 310 and 316 was investigated as a function of test temperature in boiling saturated magnesium chloride solution (MgCl2) using a constant load method. Both of types 304 and 316 exhibited similar corrosion elongation curves, while the corrosion elongation curve of type 310 was different from those of types 304 and 316, in terms of the three parameters such as time to failure (t(f)), steady-state elongation rate (l(ss)) and transition time to time to failure ratio (t(ss)/t(f)) obtained from the corrosion elongation curves for these stainless steels. The relationship between the time to failure and a reciprocal cf test temperature fell in two straight lines on a semi-logarithmic scale as well as the relationship between the steadystate elongation rate and a reciprocal of test temperature. These regions were considered to correspond to a SCC-dominated region and a hydrogen embrittlement (HE)-dominated region from the value of (t(ss)/t(f)) and the fracture appearance. The relationship between the steady state elongation rates versus time to failure on a logarithmic scale became a straight line, whereas the slopes of the line for the stainless steels were different with the different fracture mechanism iuch as SCC and HE. It was found that the linearity of the relationship can be used to predict the time to failure for the stainless steels in the corrosive environment. In addition, type 310 did not suffer from HE, which means that type 310 showed only SCC. This would be explained by whether or not a formation of alpha'-martensite takes place. (c) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:4283 / 4293
页数:11
相关论文
共 46 条
  • [11] SCC ANALYSIS OF AUSTENITIC STAINLESS-STEELS IN CHLORIDE-BEARING WATER BY NEURAL NETWORK TECHNIQUES
    SMETS, HMG
    BOGAERTS, WFL
    CORROSION, 1992, 48 (08) : 618 - 623
  • [12] Effect of residual stress on the stress corrosion cracking in boiling magnesium chloride solution of austenite stainless steel
    Wu, Huanchun
    Li, Chengtao
    Fang, Kewei
    Zhang, Wenqian
    Xue, Fei
    Zhang, Guodong
    Wang, Xuelin
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2018, 69 (11): : 1572 - 1583
  • [13] Stress corrosion cracking and life prediction of austenitic stainless steels in calcium chloride solution
    Leinonen, H
    Virkkunen, I
    Hänninen, H
    HYDROGEN EFFECTS ON MATERIAL BEHAVIOR AND CORROSION DEFORMATION INTERACTIONS, 2003, : 673 - 682
  • [14] Effect of mechanical pretreatment on gas nitriding behavior of austenitic stainless steels
    Sueyoshi, H
    Hamaishi, K
    Nakamura, Y
    Kiyofuji, J
    MATERIALS TRANSACTIONS JIM, 1996, 37 (02): : 150 - 156
  • [15] Stress corrosion cracking and life prediction evaluation of austenitic stainless steels in calcium chloride solution
    Leinonen, H
    CORROSION, 1996, 52 (05) : 337 - 346
  • [16] Residual Stress in Stainless Steels after Surface Grinding and its Effect on Chloride Induced SCC
    Zhou, Nian
    Peng, Ru Lin
    Pettersson, Rachel
    Schonning, Mikael
    RESIDUAL STRESSES 2016: ICRS-10, 2017, 2 : 289 - 294
  • [17] Surface buffing and its effect on chloride induced SCC of 304L austenitic stainless steel
    Kumar, Pandu Sunil
    Acharyya, Swati Ghosh
    Rao, S. V. Ramana
    Kapoor, Komal
    INTERNATIONAL CONFERENCE ON ADVANCES IN METALLURGY, MATERIALS AND MANUFACTURING, 2018, 314
  • [18] Nitrogen effect on hydrogen diffusivity and hydrogen embrittlement behavior in austenitic stainless steels
    Kim, Kyung-Shik
    Kang, Jee-Hyun
    Kim, Sung-Joon
    SCRIPTA MATERIALIA, 2020, 184 (184) : 70 - 73
  • [19] EFFECT OF MECHANICAL PRETREATMENT ON GAS NITRIDING BEHAVIOR IN AUSTENITIC STAINLESS-STEELS
    HAMAISHI, K
    SUEYOSHI, H
    KIYOFUJI, J
    NAKAMURA, Y
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1995, 59 (02) : 133 - 139
  • [20] Impact of temperature excursion on stress corrosion cracking of stainless steels in chloride solution
    Turnbull, A.
    Zhou, S.
    CORROSION SCIENCE, 2008, 50 (04) : 913 - 917