Effect of surface mechanical attrition treatment on corrosion fatigue behavior of AZ31B magnesium alloy

被引:50
作者
Chen, Gang [1 ]
Fu, Yuanjie [1 ]
Cui, Yun [2 ]
Gao, Jianwen [1 ]
Guo, Xiang [3 ,4 ]
Gao, Hong [1 ]
Wu, Suzhou [5 ,6 ]
Lu, Jian [5 ,6 ]
Lin, Qiang [1 ]
Shi, Shouwen [1 ]
机构
[1] Tianjin Univ, Sch Chem Engn & Technol, Tianjin 300072, Peoples R China
[2] Tianjin Univ, Sch Chem Engn & Technol, Renai Coll, Tianjin, Peoples R China
[3] Tianjin Univ, Sch Mech Engn, Tianjin, Peoples R China
[4] Tianjin Key Lab Nonlinear Dynam & Control, Tianjin 300072, Peoples R China
[5] City Univ Hong Kong, Dept Mech & Biomed Engn, Kowloon, Hong Kong, Peoples R China
[6] City Univ Hong Kong Shenzhen, Res Inst, Ctr Adv Struct Mat, 8 Yuexing 1st Rd, Shenzhen, Peoples R China
基金
中国国家自然科学基金;
关键词
Fatigue; Corrosion fatigue; Magnesium alloy; Surface mechanical attrition treatment; NaCl environment; CYCLIC AXIAL LOAD; MG ALLOY; RATCHETING BEHAVIOR; FAILURE BEHAVIORS; STAINLESS-STEEL; RECENT PROGRESS; WORK FUNCTION; STRAIN-RATE; NANOCRYSTALLIZATION; RESISTANCE;
D O I
10.1016/j.ijfatigue.2019.06.031
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Surface mechanical attrition treatment (SMAT) is considered as an effective technology to influence fatigue and corrosion resistance as these properties are largely related to surface structure and property. Despite the increasing number of studies that report the effects of SMAT on separate fatigue or corrosion behaviors, the impact of SMAT on fatigue property under corrosive environment is left unexplored. In this paper, the corrosion fatigue properties of AZ31B magnesium alloy before and after SMAT process are investigated. Hydrogen evolution tests and potentiodynamic polarization tests are carried out to obtain the corrosion resistance, and it is found that SMAT promotes corrosion rate. The surface roughness of SMATed specimen also increases, which accelerates corrosion rate. In terms of fatigue properties, the fatigue life of SMATed specimen is found to be higher, in both air and 3% NaCl solution. And the larger the size of stainless steel balls used during processing SMAT specimens, the longer the fatigue life. Under 3% NaCl corrosive environment, the beneficial effects induced by SMAT process gradually emerge with increasing stress amplitude during fatigue tests. Reduced fatigue life of SMATed specimen under corrosive environment is attributed to roughened interface between deformed surface layer and bulk material. Nevertheless, the crack initiation sites for SMAT specimens are the same in both air and NaCl solution, all located at the subsurface area.
引用
收藏
页码:461 / 469
页数:9
相关论文
共 52 条
[1]   Investigating the effects of bulk and surface severe plastic deformation on the fatigue, corrosion behaviour and corrosion fatigue of AA5083 [J].
Abdulstaar, Mustafa ;
Mhaede, Mansour ;
Wollmann, Manfred ;
Wagner, Lothar .
SURFACE & COATINGS TECHNOLOGY, 2014, 254 :244-251
[2]   The effect of combined shot-peening and PEO treatment on the corrosion performance of 2024 Al alloy [J].
Asquith, D. T. ;
Yerokhin, A. L. ;
Yates, J. R. ;
Matthews, A. .
THIN SOLID FILMS, 2007, 516 (2-4) :417-421
[3]   Influence of surface mechanical attrition treatment (SMAT) on the corrosion behaviour of AISI 304 stainless steel [J].
Balusamy, T. ;
Narayanan, T. S. N. Sankara ;
Ravichandran, K. ;
Park, Il Song ;
Lee, Min Ho .
CORROSION SCIENCE, 2013, 74 :332-344
[4]   Effect of surface nanocrystallization on the corrosion behaviour of AISI 409 stainless steel [J].
Balusamy, T. ;
Kumar, Satendra ;
Narayanan, T. S. N. Sankara .
CORROSION SCIENCE, 2010, 52 (11) :3826-3834
[5]   Corrosion fatigue behavior of extruded magnesium alloy AZ80-T5 in a 5% NaCl environment [J].
Bhuiyan, Md Shahnewaz ;
Mutoh, Yoshiharu ;
Murai, Tsutomu ;
Iwakami, Shinpei .
ENGINEERING FRACTURE MECHANICS, 2010, 77 (10) :1567-1576
[6]   Corrosion fatigue behavior of conversion coated AZ61 magnesium alloy [J].
Bhuiyan, Md. Shahnewaz ;
Ostuka, Yuichi ;
Mutoh, Yoshiharu ;
Murai, Tsutomu ;
Iwakami, Shinpei .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (18-19) :4978-4984
[7]   Corrosion behaviour of stressed magnesium alloys [J].
Bonora, PL ;
Andrei, M ;
Eliezer, A ;
Gutman, EM .
CORROSION SCIENCE, 2002, 44 (04) :729-749
[8]   Optimization of the strain rate to achieve exceptional mechanical properties of 304 stainless steel using high speed ultrasonic surface mechanical attrition treatment [J].
Chan, H. L. ;
Ruan, H. H. ;
Chen, A. Y. ;
Lu, J. .
ACTA MATERIALIA, 2010, 58 (15) :5086-5096
[9]   Multiaxial ratcheting behavior of zirconium alloy tubes under combined cyclic axial load and internal pressure [J].
Chen, G. ;
Zhang, X. ;
Xu, D. K. ;
Li, D. H. ;
Chen, X. ;
Zhang, Z. .
JOURNAL OF NUCLEAR MATERIALS, 2017, 489 :99-108
[10]   Effects of strain rate on the low cycle fatigue behavior of AZ31B magnesium alloy processed by SMAT [J].
Chen, Gang ;
Gao, Jianwen ;
Cui, Yun ;
Gao, Hong ;
Guo, Xiang ;
Wu, Suzhou .
JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 735 :536-546