Intrinsic static strength of friction interfaces augmented with anaerobic adhesives

被引:51
作者
Dragoni, E
Mauri, P
机构
[1] Univ Bologna, Dipartimento Meccan, I-40136 Bologna, Italy
[2] Loctite Italis SPA, I-20047 Brugherio, MI, Italy
关键词
friction; anaerobics; metals; joint design; static strength;
D O I
10.1016/S0143-7496(99)00062-7
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The paper is focused on the static strength of friction joints supplemented with anaerobic adhesives. Through torsional tests on the annular interface between tubular steel specimens, the friction and the adhesive contributions to the overall strength are determined as a function of the clamping force. The analysis shows no interaction of the component strengths, with the frictional strength proportional to and the adhesive strength independent of the clamping force as if the underlying mechanisms were acting separately. This cumulative performance, intrinsic of the interface in the homogeneous test conditions attained, should be exploited to the full when designing efficient real joints based on this hybrid technology. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:315 / 321
页数:7
相关论文
共 15 条
[11]  
NIEMANN G, 1981, MASCHINEN ELEMENTE, V1
[12]  
OREILLY C, 1990, SAE INT C EXP DETR 2
[13]   SYMMETRIC LAP-SHEAR TEST - WHAT GOOD IS IT [J].
RENTON, WJ .
EXPERIMENTAL MECHANICS, 1976, 16 (11) :409-415
[14]  
ROMANOS G, 1997, MECH BEHAV ADHESIVE
[15]  
WERTH S, 1938, VDI Z, V82, P471