In vitro degradation of porous poly(DL-lactide-co-glycolide) (PLGA)/bioactive glass composite foams with a polar structure

被引:34
|
作者
Orava, Eeva
Korventausta, Joni
Rosenberg, Meri
Jokinen, Mika
Rosling, Ari
机构
[1] Abo Akad Univ, Lab Polymer Technol, FIN-20500 Turku, Finland
[2] Univ Turku, Turku Ctr Biomat, Inst Dent, FIN-20520 Turku, Finland
[3] Univ Turku, Inst Dent, Dept Prosthet Dent, FIN-20520 Turku, Finland
关键词
degradable polymers; bioactive glass; composite; weight loss; porosity;
D O I
10.1016/j.polymdegradstab.2006.10.004
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
In vitro degradation of porous 50/50, 70/30 and 90/10 PLGA (poly(DL-lactide-co-glycolide)) foams and PLGA/bioactive glass (20 wt%) composite foams was studied up to 16 weeks in TRIS (PH 7.4; 37 degrees C). Polar PLGA/bioactive glass composite films were prepared by applying the bioactive glass (S53P4) on one side of the composite. Porous foams were made by solvent casting and pressure quenching with CO2. The fabricated foams had an initial pore size of 50-500 mu m and thickness of 2-2.5 mm. In vitro degradation of the prepared foams was evaluated after 1, 2, 4, 6, 8, 12 and 16 weeks. Weight loss, water uptake, molecular mass and the amount of dissolved bioactive glass were measured after each time period. Changes in pore morphology were analysed with SEM. The present in vitro results will be evaluated and compared with the results from ongoing animal studies where comparable implants are used for bone defect treatment under non-load-bearing conditions. (c) 2006 Elsevier Ltd. All rights reserved.