Degradation of silicone polymer in a field soil under natural conditions

被引:63
作者
Lehmann, RG [1 ]
Miller, JR [1 ]
Kozerski, GE [1 ]
机构
[1] Dow Corning Corp, Hlth & Environm Sci, Midland, MI 48686 USA
关键词
silicone; polydimethylsiloxane; degradation; soil; environment;
D O I
10.1016/S0045-6535(99)00430-0
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Silicone polymers (PDMS = polydimethylsiloxane) are used in numerous consumer and industrial products. Our previous work showed that they will degrade in soil under laboratory conditions. This paper investigates PDMS degradation in the field. Four soil plots (each 2.44 m x 2.44 m) in Michigan were sprayed in May, 1997, with aqueous emulsion to achieve nominal soil PDMS concentrations of 0 (control), 215 (low), 430 (medium), and 860 (high) mu g/g. Over the following summer, soil cores (0-5 and 5-10 cm) were collected every two weeks and analyzed for decrease in total soil PDMS, and decrease in molecular weight of remaining PDMS. PDMS concentrations decreased 50% in 4.5, 5.3, and 9.6 weeks for the low, medium, and high treatments, respectively. Degradation rates were 0.26 (low), 0.44 (medium), and 0.44 (high) g PDMS/m(2) day, indicating that degradation capacity of the soil was exceeded by the High treatment. Dimethylsilanediol (DMSD), the main degradation product, was detected in most samples at <5% of original PDMS. This is consistent with laboratory data showing biodegradation and volatilization of DMSD. Deeper sampling (to 20 cm) found only trace amounts of DMSD, and minor downward movement of the polymer. Respraying and subsequent analysis of one plot with a medium treatment in late August showed slow PDMS degradation during the cool, wet fall, followed by a 40% decrease over winter and extensive degradation during the summer of 1998. The study thus shows that PDMS will degrade under field conditions as predicted from laboratory experiments. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:743 / 749
页数:7
相关论文
共 26 条
[1]   KINETICS OF THE GAS-PHASE REACTIONS OF A SERIES OF ORGANOSILICON COMPOUNDS WITH OH AND NO3 RADICALS AND O-3 AT 297 +/- 2-K [J].
ATKINSON, R .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 1991, 25 (05) :863-866
[2]   REARRANGEMENT OF POLY(DIMETHYLSILOXANE) FLUIDS ON SOIL [J].
BUCH, RR ;
INGEBRIGTSON, DN .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 1979, 13 (06) :676-679
[3]   STUDY OF THE DEGRADATION OF POLYDIMETHYLSILOXANES ON SOIL [J].
CARPENTER, JC ;
CELLA, JA ;
DORN, SB .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 1995, 29 (04) :864-868
[4]   DEVELOPMENT OF A HIGH-PERFORMANCE LIQUID-CHROMATOGRAPHIC INDUCTIVELY-COUPLED PLASMA METHOD FOR SPECIATION AND QUANTIFICATION OF SILICONES - FROM SILANOLS TO POLYSILOXANES [J].
DORN, SB ;
FRAME, EMS .
ANALYST, 1994, 119 (08) :1687-1694
[5]  
GARWOOD A. N., 1996, WEATHER AM
[6]  
HUTCHISON DE, 1979, SOIL SURVEY MIDLAND
[7]  
LEHMANN RG, 1994, ENVIRON TOXICOL CHEM, V13, P1753, DOI [10.1897/1552-8618(1994)13[1753:FOSDPS]2.0.CO
[8]  
2, 10.1002/etc.5620131106]
[9]   Microbial degradation of dimethylsilanediol in soil [J].
Lehmann, RG ;
Miller, JR ;
Collins, HP .
WATER AIR AND SOIL POLLUTION, 1998, 106 (1-2) :111-122
[10]  
Lehmann RG, 1996, ENVIRON TOXICOL CHEM, V15, P1455, DOI [10.1002/etc.5620150905, 10.1897/1551-5028(1996)015&lt