共 50 条
Oxygen Reduction Reaction Activity of Carbon-Supported Pt-Fe, Pt-Co, and Pt-Ni Alloys with Stabilized Pt-Skin Layers
被引:39
|作者:
Chiwata, Morio
[1
]
Yano, Hiroshi
[2
]
Ogawa, Satoshi
[1
]
Watanabe, Masahiro
[2
]
Iiyama, Akihiro
[2
]
Uchida, Hiroyuki
[2
,3
]
机构:
[1] Univ Yamanashi, Interdisciplinary Grad Sch Med & Engn, Takeda 4, Kofu, Yamanashi 4008510, Japan
[2] Univ Yamanashi, Fuel Cell Nanomat Ctr, Takeda 4, Kofu, Yamanashi 4008510, Japan
[3] Univ Yamanashi, Clean Energy Res Ctr, Takeda 4, Kofu, Yamanashi 4008510, Japan
关键词:
Polymer Electrolyte Fuel Cell;
Electrocatalyst;
Pt alloy;
Oxygen Reduction Reaction;
TEMPERATURE-DEPENDENCE;
NANOCAPSULE METHOD;
BLACK CATALYSTS;
PARTICLE-SIZE;
ELECTROCATALYSTS;
PLATINUM;
ENHANCEMENT;
ELECTRODE;
PEMFCS;
D O I:
10.5796/electrochemistry.84.133
中图分类号:
O646 [电化学、电解、磁化学];
学科分类号:
081704 ;
摘要:
We have prepared carbon-supported Pt-M (M = Fe, Co, and Ni) alloy nanoparticles with uniform size and composition as cathode catalysts for polymer electrolyte fuel cells. In order to protect the underlying Pt-M alloy from dealloying and maintain high mass activity for the oxygen reduction reaction (ORR), two atomic layers of Pt-skin (Pt-2AL) were formed on the Pt-M nanopartcicles. By means of various types of analysis, including X-ray diffraction (XRD), inductively coupled plasma mass analysis (ICP-MS), thermogravimetry (TG), and transmission electron microscopy (TEM), the formation of monodisperse Pt-2AL-Pt-M/C was confirmed. The kinetically-controlled ORR activities (mass activity, MA(k), and area-specific activity, j(k)) for the ORR at Nafion (R)-coated Pt-2AL-Pt-M/C catalysts in O-2-saturated 0.1 M HClO4 solution were evaluated by the use of a multi-channel flow double electrode cell at 65 degrees C. It was found that the initial value of MA(k) at Pt-2AL-PtNi/C was the highest, i.e., 3.3 times higher than that at a commercial catalyst, carbon-supported Pt (c-Pt/C). In contrast, the Pt-2AL-PtCo/C catalyst exhibited superior durability, so that dealloying was almost entirely suppressed, together with a great mitigation of the particle agglomeration after applying 10(4) cycles of potential steps between 0.6V and 1.0 V. (C) The Electrochemical Society of Japan, All rights reserved.