Comparative Study of the Effect of Different Nanoparticles on the Mechanical Properties, Permeability, and Thermal Degradation Mechanism of HDPE

被引:95
作者
Chrissafis, K. [1 ]
Paraskevopoulos, K. M. [1 ]
Tsiaoussis, I. [1 ]
Bikiaris, D. [2 ]
机构
[1] Aristotle Univ Thessaloniki, Dept Phys, Solid State Phys Sect, GR-54124 Thessaloniki, Macedonia, Greece
[2] Aristotle Univ Thessaloniki, Lab Organ Chem Technol, Dept Chem, GR-54124 Thessaloniki, Macedonia, Greece
关键词
nanocomposites; polyethylene; multiwalled carbon nanotubes; montmorillonite; fumed silica; thermal stability; gas permeability; HIGH-DENSITY POLYETHYLENE; ISOTACTIC POLYPROPYLENE/SIO2 NANOCOMPOSITES; GAS PERMEATION PROPERTIES; WALLED CARBON NANOTUBES; PP-G-MA; PHYSICAL-PROPERTIES; KINETIC-PARAMETERS; DTG CURVE; CLAY; MORPHOLOGY;
D O I
10.1002/app.30750
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
In the present study, different series of high-density polyethylene (HDPE) nanocomposites were prepared by melt mixing on a Haake-Buchler Reomixer, containing 2.5 wt % of multiwall carbon nanotubes, pristine and modified montmorillonite, surface-treated and untreated SiO2 nanoparticles. From transmission electron micrographs, it was found that beyond a fine dispersion of nanoparticles into HDPE matrix, there are also some aggregates easily discriminated. As a result, there was a decrease in the tensile and impact strength of most of nanocomposites except Young's modulus, which was increased. Storage modulus as recorded from dynamic mechanical analysis was also increased in all nanocomposites, because HDPE becomes stiffer due to the incorporation of nanoparticles. The nucleation behavior of nanoparticles during crystallization was found to have no obvious effect on melting and crystallization temperature of HDPE. However, a small decrease in the heat of fusion in all nanocomposites was evidenced. Gas permeability of HDPE matrix in O-2, N-2, and CO2 was reduced in all nanocomposites compared with neat polymer. Thermal stability of HDPE was also enhanced due to the incorporation of different nanoparticles. From the kinetic analysis of thermal decomposition of HDPE, it was concluded that to describe the thermal degradation of HDPE and the studied nanocomposites, two consecutive mechanisms of nth-order autocatalysis have to be considered. (C) 2009 Wiley Periodicals, Inc. J Appl Polym Sci 114: 1606-1618, 2009
引用
收藏
页码:1606 / 1618
页数:13
相关论文
共 65 条
[1]  
ARAUJO AS, 2002, THERMOCHIM ACTA, V55, P392
[2]   A kinetic approach to the temperature-programmed pyrolysis of low- and high-density polyethylene in a fixed bed reactor:: determination of kinetic parameters for the evolution of n-paraffins and 1-olefins [J].
Ballice, L .
FUEL, 2001, 80 (13) :1923-1935
[3]   Effect of acid treated multi-walled carbon nanotubes on the mechanical, permeability, thermal properties and thermo-oxidative stability of isotactic polypropylene [J].
Bikiaris, D. ;
Vassiliou, A. ;
Chrissafis, K. ;
Paraskevopoulos, K. M. ;
Jannakoudakis, A. ;
Docoslis, A. .
POLYMER DEGRADATION AND STABILITY, 2008, 93 (05) :952-967
[4]   Compatibilisation effect of PP-g-MA copolymer on iPP/SiO2 nanocomposites prepared by melt mixing [J].
Bikiaris, DN ;
Vassiliou, A ;
Pavlidou, E ;
Karayannidis, GP .
EUROPEAN POLYMER JOURNAL, 2005, 41 (09) :1965-1978
[5]   Preparation bv melt mixing and characterization of isotactic polypropylene/SiO2 nanocomposites containing untreated and surface-treated nanoparticles [J].
Bikiaris, DN ;
Papageorgiou, GZ ;
Pavlidou, E ;
Vouroutzis, N ;
Palatzoglou, P ;
Karayannidis, GP .
JOURNAL OF APPLIED POLYMER SCIENCE, 2006, 100 (04) :2684-2696
[6]   Mechanisms and kinetics of thermal decomposition of plastics from isothermal and dynamic measurements [J].
Bockhorn, H ;
Hornung, A ;
Hornung, U .
JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 1999, 50 (02) :77-101
[7]   Kinetic study on the thermal degradation of polypropylene and polyethylene [J].
Bockhorn, H ;
Hornung, A ;
Hornung, U ;
Schwaller, D .
JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 1999, 48 (02) :93-109
[8]   Characterization and thermal degradation mechanism of isotactic polypropylene/carbon black nanocomposites [J].
Chrissafis, K. ;
Paraskevopoulos, K. M. ;
Stavrev, S. Y. ;
Docoslis, A. ;
Vassiliou, A. ;
Bikiaris, D. N. .
THERMOCHIMICA ACTA, 2007, 465 (1-2) :6-17
[9]   Comparative study of the effect of different nanoparticles on the mechanical properties and thermal degradation mechanism of in situ prepared poly(E-caprolactone) nanocomposites [J].
Chrissafis, K. ;
Antoniadis, G. ;
Paraskevopoulos, K. M. ;
Vassiliou, A. ;
Bikiaris, D. N. .
COMPOSITES SCIENCE AND TECHNOLOGY, 2007, 67 (10) :2165-2174
[10]   Thermal degradation kinetics of the biodegradable aliphatic polyester, poly(propylene succinate) [J].
Chrissafis, K ;
Paraskevopoulos, KM ;
Bikiaris, DN .
POLYMER DEGRADATION AND STABILITY, 2006, 91 (01) :60-68