Influence of repetitions of the high-pressure hydrogen gas exposure on the internal damage quantity of high-density polyethylene evaluated by transmitted light digital image

被引:34
|
作者
Ono, Hiroaki [1 ]
Fujiwara, Hirotada [1 ]
Onoue, Kiyoaki [1 ]
Nishimura, Shin [1 ,2 ]
机构
[1] Kyushu Univ, Res Ctr Hydrogen Ind Use & Storage HYDROGENIUS, Nishi Ku, 744 Motooka, Fukuoka, Fukuoka 8190395, Japan
[2] Kyushu Univ, Fac Engn, Dept Mech Engn, Fukuoka, Fukuoka, Japan
关键词
HDPE; Fracture; Light; Transmission; XDF; Blister; MICROCELLULAR FOAM; POLYMERIC FOAMS; DECOMPRESSION; CAVITATION; CRYSTALLINITY; NUCLEATION; SCATTERING; COLLAPSE; STATIONS; BEHAVIOR;
D O I
10.1016/j.ijhydene.2019.07.035
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
A quantitative evaluation of the bulk damage level after high-pressure hydrogen exposure for the hydrogen compatible polymeric materials are developed. The bulk damage level of the internal damage induced by high-density polyethylene (HDPE) after 90 MPa hydrogen exposure repetition were evaluated. Based on the light scattering by the internal damage, we established a quantitative damage index in terms of the light transmittance as brightness (B) of transmitted light digital image of the HDPE disk specimen; the relative extinction ratio of transmitted light intensity (beta(r)) as the brightness change ratio. beta(r) was obtained for each pixel of the image for whole specimen. According to the results of the Light specimen, beta(r) around the central region of specimen was higher than that of the edge region. Averaged beta(r) around the center of specimen ((beta(r)) over bar) logarithmically increased with the XDF increase in exposure number (N-ex). Judging from the results, the internal damage tends to Blister generate at the center of specimen, and the internal damage amount increased with in- crease in N-ex. (C) 2019 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.