Predicting the lifetime of fluorosilicone o-rings

被引:60
作者
Bernstein, R. [1 ]
Gillen, K. T. [1 ]
机构
[1] Sandia Natl Labs, Organ Mat Dept, Albuquerque, NM 87185 USA
关键词
o-Ring; Fluorosilicone; Arrhenius evaluation; Field aging; Compression set; Sealing force; NON-ARRHENIUS BEHAVIOR; DEGRADATION; EXTRAPOLATION; TEMPERATURE; RELAXATION;
D O I
10.1016/j.polymdegradstab.2009.10.005
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Long-term (up to 1000 days) accelerated oven-aging studies on a commercial fluorosilicone o-ring seal are used to predict the sealing lifetime at room temperature (23 degrees C). The study follows force decay (relaxation) on squeezed o-ring material using isothermal compression stress relaxation (CSR) techniques. The relaxation is normally a complex mix of reversible physical effects and non-reversible chemical effects but we utilize an over-strain approach to quickly achieve physical equilibrium. This allows us to concentrate the measurements on the chemical relaxation effects of primary interest to lifetime assessment. The long-term studies allow us to access a fairly broad temperature range (80-138 degrees C) which results in improved modeling of the temperature dependence of the accelerated data. Non-Arrhenius behavior is observed with evidence of a significant lowering of the activation energy at the lowest accelerated aging temperature (80 degrees C). This observation is consistent with numerous recent accelerated aging studies that probed temperature ranges large enough to observe similar non-Arrhenius behavior. The extrapolated predictions imply that significant loss of sealing force requires on the order of 50-100 years at 23 degrees C. Field aging results out to similar to 25 years at 23 degrees C are shown to be in reasonable accord with the significant change in Arrhenius slope observed from the accelerated aging study. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2107 / 2113
页数:7
相关论文
共 29 条
[1]  
Bernstein B. S., 1975, Proceedings of the 24th International Wire and Cable Symposium, P202
[2]  
BERNSTEIN R, 2007, SAND20076781
[3]   Accelerated aging and lifetime prediction: Review of non-Arrhenius behaviour due to two competing processes [J].
Celina, M ;
Gillen, KT ;
Assink, RA .
POLYMER DEGRADATION AND STABILITY, 2005, 90 (03) :395-404
[4]   Thermal degradation studies of a polyurethane propellant binder [J].
Celina, M ;
Graham, AC ;
Gillen, KT ;
Assink, RA ;
Minier, LM .
RUBBER CHEMISTRY AND TECHNOLOGY, 2000, 73 (04) :678-693
[5]   A THEORETICAL BASIS FOR VISCOELASTIC RELAXATION OF ELASTOMERS IN THE LONG-TIME LIMIT [J].
CURRO, JG ;
PINCUS, P .
MACROMOLECULES, 1983, 16 (04) :559-562
[6]  
CURRO JG, 1973, RUBBER CHEM TECHNOL, V46, P530
[7]  
Ferry J. D., 1961, Viscoelastic properties of polymers
[8]   THE INFLUENCE OF TEMPERATURE AND CATALYST RESIDUES ON THE DEGRADATION OF UNSTABILIZED POLYPROPYLENE [J].
GIJSMAN, P ;
HENNEKENS, J ;
VINCENT, J .
POLYMER DEGRADATION AND STABILITY, 1993, 39 (03) :271-277
[9]   Lifetime predictions of EPR materials using the Wear-out approach [J].
Gillen, K. T. ;
Celina, M. ;
Bernstein, R. ;
Shedd, M. .
POLYMER DEGRADATION AND STABILITY, 2006, 91 (12) :3197-3207
[10]   Lifetime predictions for semi-crystalline cable insulation materials: I. Mechanical properties and oxygen consumption measurements on EPR materials [J].
Gillen, K. T. ;
Bernstein, R. ;
Clough, R. L. ;
Celina, M. .
POLYMER DEGRADATION AND STABILITY, 2006, 91 (09) :2146-2156