Correlation between microstructure and hardness of a low activation ferritic steel (JLF-1) weld joint

被引:24
作者
Inoue, N [1 ]
Muroga, T [1 ]
Nishimura, A [1 ]
Motojima, O [1 ]
机构
[1] Natl Inst Fus Sci, Gifu 5095292, Japan
关键词
D O I
10.1016/S0022-3115(98)00291-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fe-Cr-W ferritic steels are candidate low activation materials for fusion reactor structural components. Under a surveillance test program of the Japanese low activation Fe-9Cr-2WVTa steel (JLF-1), JLF-1-HEAT2 was made by Japanese universities. The present paper reports the results of microstructural observation and hardness testing of JLF-1-HEAT2 and its weld joint. The relation of microstructure with local hardness and tensile properties at various positions on the weld joint was investigated, and the correlation qualitatively interpreted in terms of the martensitic lath width. (C) 1998 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:1248 / 1252
页数:5
相关论文
共 3 条
[1]   R-AND-D OF LOW-ACTIVATION FERRITIC STEELS FOR FUSION IN JAPANESE UNIVERSITIES [J].
KOHYAMA, A ;
KOHNO, Y ;
ASAKURA, K ;
KAYANO, H .
JOURNAL OF NUCLEAR MATERIALS, 1994, 212 :684-689
[2]   Low-activation ferritic and martensitic steels for fusion application [J].
Kohyama, A ;
Hishinuma, A ;
Gelles, DS ;
Klueh, RL ;
Dietz, W ;
Ehrlich, K .
JOURNAL OF NUCLEAR MATERIALS, 1996, 233 :138-147
[3]   INFLUENCE OF THE LATH MORPHOLOGY ON THE YIELD STRESS AND TRANSITION-TEMPERATURE OF MARTENSITIC-BAINITIC STEELS [J].
NAYLOR, JP .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1979, 10 (07) :861-873