On Mechanical Response of Aluminum Alloys in Corrosive Environment

被引:0
作者
Kumar, Sunil S. [1 ,2 ]
Londe, Neelakantha, V [2 ]
Kumar, Dilip K. [3 ]
Kittur, M., I [4 ]
Badruddin, Irfan Anjum [5 ]
Faheem, Mohammed [6 ]
Khan, Sher Afghan [6 ]
机构
[1] AJ Inst Engn & Technol, Dept Mech Engn, Mangalore 575006, Karnataka, India
[2] Mangalore Inst Technol & Engn, Dept Mech Engn, Moodabidri 574225, Karnataka, India
[3] Shree Devi Inst Technol, Dept Mech Engn, Mangalore 574142, Karnataka, India
[4] Univ Malaya, Fac Engn, Dept Mech Engn, Kuala Lumpur 50603, Malaysia
[5] King Khalid Univ, Coll Engn, Dept Mech Engn, Abha 61421, Saudi Arabia
[6] Int Islamic Univ Malaysia, Dept Mech Engn, Kuala Lumpur 50728, Malaysia
来源
INTERNATIONAL JOURNAL OF INTEGRATED ENGINEERING | 2022年 / 14卷 / 01期
关键词
Aluminum alloys; pitting; corrosion; mechanical properties; SALT-SPRAY; PITTING CORROSION; BEHAVIOR; STEEL; TENSILE; MICROSTRUCTURE; STRENGTH; IMPACT; AL;
D O I
10.30880/ijie.2022.14.01.005
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Al6061T6 and Al7075T6 aluminum alloys are subjected to accelerated salt spray corrosion to evaluate the amount of degradation and the effect on mechanical behavior. The specimens were stored in a closed chamber with continuous salt spray for a period of 250 hours and 500 hours, respectively. It was observed that the oxide layer was unprotective after prolonged salt spray resulting in pitting continued with exfoliation corrosion. The tensile test results show that there was a remarkable decrease in tensile properties with exposure time. A significant reduction in tensile strength, yield strength, elongation at yield, elongation at break, and overall toughness in both the alloys was observed at 500 hours. The impact strength decreased by 14.4 % and 26.47 %, Rockwell hardness (HRB) reduced by 12.2% and 20.71% for respective alloys at 500 hours of exposure. However, there was an increasing trend in elastic stiffness which attributed to decrease in ductility. Furthermore, it was comparatively observed that Al7075T6 is more susceptible to corrosion than Al6061T6.
引用
收藏
页码:48 / 56
页数:9
相关论文
共 35 条
[1]   Effect of corrosion-induced hydrogen embrittlement and its degradation impact on tensile properties and fracture toughness of (Al-Cu-Mg) 2024 alloy [J].
Alexopoulos, Nikolaos D. ;
Dietzel, Wolfgang .
21ST EUROPEAN CONFERENCE ON FRACTURE, (ECF21), 2016, 2 :573-580
[2]  
[Anonymous], 2015, ASTM E 18-15
[3]  
[Anonymous], 2018, ASTM E-23
[4]  
[Anonymous], 2016, E8 ASTM
[5]  
[Anonymous], 2011, ASTM B117-11
[6]   Mechanical behavior of corroded reinforcing steel bars S500s tempcore under low cycle fatigue [J].
Apostolopoulos, Ch. Alk. .
CONSTRUCTION AND BUILDING MATERIALS, 2007, 21 (07) :1447-1456
[7]   Tensile behavior of corroded reinforcing steel bars BSt 500s [J].
Apostolopoulos, Ch. Alk. ;
Papadopoulos, M. P. ;
Pantelakis, Sp. G. .
CONSTRUCTION AND BUILDING MATERIALS, 2006, 20 (09) :782-789
[8]   The relation between microstructure and corrosion behavior of Mg-Y-RE-Zr alloys [J].
Ben-Hamu, G. ;
Eliezer, D. ;
Shin, K. S. ;
Cohen, S. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2007, 431 (1-2) :269-276
[9]   Exfoliation Corrosion Impact on Microstructure, Mechanical Properties, and Fatigue Crack Growth of Aeronautical Aluminum Alloy [J].
Brahami, Abdessamad ;
Fajoui, Jamel ;
Bouchouicha, Benattou .
JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2020, 20 (01) :197-207
[10]   Failure behaviour of SPR joints after salt spray test [J].
Calabrese, L. ;
Proverbio, E. ;
Di Bella, G. ;
Galtieri, G. ;
Borsellino, C. .
ENGINEERING STRUCTURES, 2015, 82 :33-43