Analysis of the creep behavior of fine-grained AZ31 magnesium alloy

被引:27
作者
Figueiredo, Roberto B. [1 ]
Langdon, Terence G. [2 ,3 ,4 ]
机构
[1] Univ Fed Minas Gerais, Dept Met & Mat Engn, BR-31270901 Belo Horizonte, MG, Brazil
[2] Univ Southampton, Dept Mech Engn, Mat Res Grp, Southampton SO17 1BJ, Hants, England
[3] Univ Southern Calif, Dept Aerosp & Mech Engn, Los Angeles, CA 90089 USA
[4] Univ Southern Calif, Dept Mat Sci, Los Angeles, CA 90089 USA
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2020年 / 787卷
基金
欧洲研究理事会;
关键词
AZ31 magnesium alloy; Creep; Deformation mechanism maps; Equal-channel angular pressing; Grain boundary sliding; HIGH-TEMPERATURE DEFORMATION; SUPERPLASTIC DUCTILITY; ELEVATED-TEMPERATURES; VISCOUS GLIDE; HCP METALS; MECHANISMS; FLOW; CAVITATION; TEXTURE;
D O I
10.1016/j.msea.2020.139489
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Double-shear creep testing was used to evaluate the creep behavior of a magnesium AZ31 alloy processed by equal-channel angular pressing to produce an average grain size of similar to 2.7 mu m. The results show that rapid creep rates are observed in the early stages of deformation due to the occurrence of grain boundary sliding in the finegrained structure but the creep rates decrease with increasing deformation due to grain growth. The stress exponent for flow in the early stages is similar to 2 and the activation energy is similar to 92 kJ mol(-1) where these values are consistent with the expectations for grain boundary sliding under superplastic conditions. Annealing the material for 24 h at 723 K before creep testing produces a significantly larger grain size of similar to 50 mu m and this prevents grain boundary sliding and leads to an increasing stress exponent at higher stresses. Deformation mechanism maps are constructed incorporating both the present experimental results for a fine-grained magnesium alloy and results from published data for the AZ31 alloy. These maps provide a useful tool for evaluating the experimental conditions that are necessary for achieving superplastic forming operations.
引用
收藏
页数:7
相关论文
共 47 条
[1]  
Ashby M.F., 1982, DEFORMATION MECH MAP
[2]  
Bird J.E., 1969, Quantitative Relation between Properties and Microstructure
[3]   CREEP CERAMICS .2. AN EXAMINATION OF FLOW MECHANISMS [J].
CANNON, WR ;
LANGDON, TG .
JOURNAL OF MATERIALS SCIENCE, 1988, 23 (01) :1-20
[5]   Superplastic forming of AZ31 magnesium alloy with controlled microstructure [J].
Cusick, M. ;
Abu-Farha, F. ;
Lours, P. ;
Maoult, Y. ;
Bernhart, G. ;
Khraisheh, M. .
MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2012, 43 (09) :810-816
[6]   Deformation mechanisms responsible for the high ductility in a Mg AZ31 alloy analyzed by electron backscattered diffraction [J].
Del Valle, JA ;
Pérez-Prado, MT ;
Ruano, OA .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2005, 36A (06) :1427-1438
[7]   Effect of temperature on deformation mechanisms of AZ31 Mg-alloy under tensile loading [J].
Dessolier, Thibaut ;
Lhuissier, Pierre ;
Roussel-Dherbey, Francine ;
Charlot, Frederic ;
Josserond, Charles ;
Blandin, Jean-Jacques ;
Martin, Guilhem .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 775
[8]   Record superplastic ductility in a magnesium alloy processed by equal-channel angular pressing [J].
Figueiredo, Roberto B. ;
Langdon, Terence G. .
ADVANCED ENGINEERING MATERIALS, 2008, 10 (1-2) :37-40
[9]   Evaluating the Superplastic Flow of a Magnesium AZ31 Alloy Processed by Equal-Channel Angular Pressing [J].
Figueiredo, Roberto B. ;
Langdon, Terence G. .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2014, 45A (08) :3197-3204
[10]   Influence of rolling direction on flow and cavitation in a superplastic magnesium alloy processed by equal-channel angular pressing [J].
Figueiredo, Roberto B. ;
Langdon, Terence G. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 556 :211-220