Fatigue Performance of Geosynthetic-Reinforced Asphalt Concrete Beams

被引:13
作者
Sudarsanan, Nithin [1 ]
Arulrajah, Arul [2 ]
Karpurapu, Rajagopal [3 ]
Amirthalingam, Veeraragavan [3 ]
机构
[1] North Carolina State Univ, Dept Civil Construct & Environm Engn, Raleigh, NC 27607 USA
[2] Swinburne Univ Technol, Dept Civil & Construct Engn, Hawthorn, Vic 3122, Australia
[3] Indian Inst Technol Madras, Dept Civil Engn, Chennai 600036, Tamil Nadu, India
关键词
Geosynthetics; Paving fabric; Four-point beam fatigue test; Fatigue life; Bond strength; Fracture energy; Geosynthetic interlayers; Natural geotextiles; LABORATORY CHARACTERIZATION; REFLECTIVE CRACKING; BEHAVIOR; OVERLAY; SYSTEMS;
D O I
10.1061/(ASCE)MT.1943-5533.0003267
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
One of the common distresses observed in asphalt concrete (AC) pavements under repeated vehicular and thermal loadings is cracking. Overlay placement is a quick remedy to rehabilitate these distressed surfaces. Unfortunately, this practice without treating the cracks will not resolve the cracking issue because the existing cracked surface soon propagates the cracks through the new layer, resulting in a phenomenon known as reflective cracking. Different types of geosynthetic interlayers have been used to retard the reflective cracks, thereby enhancing the overlay's service life. The preliminary step in quantifying the service life improvement is measuring the fatigue life enhancement in the laboratory. This paper developed a test procedure to conduct four-point beam (4PB) fatigue tests, adapted a permanent deformation evolution model (PDEM) to predict the fatigue life of the 4PB specimens under laboratory testing conditions, and compared the fatigue life of beam specimens reinforced with three types of geosynthetics at 10 degrees C, 20 degrees C, and 30 degrees C. The improvement factor measured using the PDEM model indicated that the geosynthetic reinforcement in AC beams increased the fatigue life on the order of 1.2-12 times depending upon the temperature at which the test was performed and the choice of the geosynthetic type. The best fatigue life outcome is expected when the improvement factor calculated for the geosynthetic-reinforced asphalt concrete's bond strength and fracture energy meets the right combination of threshold values. The limitation of the study is that the improvement factors evaluated from the laboratory fatigue life require calibration factors to predict the field performance. Further field studies of the geosynthetic-reinforced pavements will help establish these calibration factors.
引用
收藏
页数:13
相关论文
共 44 条
  • [1] AASHTO, 2015, AASHTOM288
  • [2] AGPT (Australasian Guide to Pavement Technology), 2006, AGPTT23306
  • [3] Laboratory characterisation of the fatigue behaviour of a glass fibre grid-reinforced asphalt concrete using 4PB tests
    Arsenie, Ioana Maria
    Chazallon, Cyrille
    Duchez, Jean-Louis
    Hornych, Pierre
    [J]. ROAD MATERIALS AND PAVEMENT DESIGN, 2017, 18 (01) : 168 - 180
  • [4] ASTM, 2010, ASTM D7460
  • [5] ASTM, 2013, D7239 ASTM
  • [6] ASTM, 2014, D6140: Standard Test Method to Determine Asphalt Retention of Paving Fabrics Used in Asphalt Paving for Full-Width Applications
  • [7] Baburamani P., 1999, ASPHALT FATIGUE LIFE
  • [8] Baek J., 2010, MODELING REFLECTIVE, P143
  • [9] Bocci M, 2007, PROC MONOGR ENG WATE, P1415
  • [10] Bognacki C. J., 2007, P WORLDW AIRP TECHN