Formation of Black Striped Oxide Scale on Hot-Rolled Si-Containing Carbon Steel

被引:2
作者
Shih, Chun-Chao [1 ,2 ]
Wu, Min-Tao [3 ]
Huang, Chao-Chi [3 ]
Hwang, Weng-Sing [2 ]
Kuo, Jui-Chao [2 ]
机构
[1] China Steel Corp, Met Dept, 1 Zhonggang Rd, Kaohsiung 81233, Taiwan
[2] Natl Cheng Kung Univ, Dept Mat Sci & Engn, 1 Univ Rd, Tainan 70101, Taiwan
[3] China Steel Corp, Iron & Steel Res & Dev Dept, 1 Zhonggang Rd, Kaohsiung 81233, Taiwan
关键词
black striped oxide scale; hydraulic descaling; overcooling; deformability; OXIDATION; IRON; TEMPERATURE; MECHANISM; SYSTEM; MODEL;
D O I
10.2320/matertrans.M2018060
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The black striped oxide scale formed on silicon (Si)-containing hot-rolled carbon steel sheets was investigated. The small black stripes of oxide scale became band shaped as the flow used in mill cooling was increased. The distance between the black oxide scale bands was the same as that of the overlapping areas in the hydraulic descaling system. The average thickness of the black striped oxide scale was larger than that of the normal scale region. No ferric oxide (Fe2O3) was observed in the scale, particularly in the fractured parts of the black striped oxide scale. Furthermore, Si did not obviously accumulate in the black striped oxide scale, indicating that the oxide scale was not induced by the residual secondary scale generated during rough milling. The cooling conditions in finish milling affected the deformability of the scale in the overlapping areas. Consequently, the difference in thickness between the overlapping areas and adjacent regions led to the formation of the black striped oxide scale.
引用
收藏
页码:1716 / 1722
页数:7
相关论文
共 20 条
[1]   Influence of Ni impurity in steel on the removability of primary scale in hydraulic descaling [J].
Asai, T ;
Soshiroda, T ;
Miyahara, M .
ISIJ INTERNATIONAL, 1997, 37 (03) :272-277
[2]   AN ASSESSMENT OF THE SYSTEM FE-O-SIO2 USING A STRUCTURE BASED MODEL FOR THE LIQUID SILICATE [J].
BJORKMAN, B .
CALPHAD-COMPUTER COUPLING OF PHASE DIAGRAMS AND THERMOCHEMISTRY, 1985, 9 (03) :271-282
[3]  
Bowen NL, 1932, AM J SCI, V24, P177
[4]   Review of the high-temperature oxidation of iron and carbon steels in air or oxygen [J].
Chen, RY ;
Yuen, WYD .
OXIDATION OF METALS, 2003, 59 (5-6) :433-468
[5]   MECHANISM OF RED SCALE DEFECT FORMATION IN SI-ADDED HOT-ROLLED STEEL SHEETS [J].
FUKAGAWA, T ;
OKADA, H ;
MAEHARA, Y .
ISIJ INTERNATIONAL, 1994, 34 (11) :906-911
[6]  
FUKAGAWA T, 1995, TETSU TO HAGANE, V81, P559
[7]  
Fukagawa T, 1996, TETSU TO HAGANE, V82, P63
[8]   Segregation across the metal/oxide interface occurring during oxidation at high temperatures of diluted iron based alloys [J].
Geneve, D. ;
Rouxel, D. ;
Weber, B. ;
Confente, M. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 435 :1-11
[9]  
Helena V., 2015, 24 INT C MET MAT OST, P1
[10]   Tensile deformation of iron oxides at 600-1250°C [J].
Hidaka, Y ;
Anraku, T ;
Otsuka, N .
OXIDATION OF METALS, 2002, 58 (5-6) :469-485