Fracture Resistance of Various Thickness e.max CAD Lithium Disilicate Crowns Cemented on Different Supporting Substrates: An In Vitro Study

被引:20
作者
Chen, Sara Elizabeth [1 ]
Park, Albert Christopher [1 ]
Wang, Jingxu [2 ]
Knoernschild, Kent L. [1 ]
Campbell, Stephen [1 ]
Yang, Bin [1 ]
机构
[1] Univ Illinois Chicago Restorat Dent, Chicago, IL 60612 USA
[2] Guangzhou Med Univ, Dept Stomatol, Affiliated Hosp 1, Guangzhou, Peoples R China
来源
JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY | 2019年 / 28卷 / 09期
关键词
Monolithic; occlusal thickness; load-bearing capacity; preparation design; all ceramic crown; ultra-thin crown;
D O I
10.1111/jopr.13108
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: To investigate the influence of abutment material properties on the fracture resistance and failure mode of lithium disilicate (IPS e.max) CAD/CAM (computer-aided design/manufacturing) crowns on traditionally and minimally prepared simulated tooth substrates. Materials and Methods: Thirty lithium disilicate (IPS e.max) CAD/CAM crowns were divided into three groups (n = 10): TD: traditional thickness crowns cemented on Paradigm MZ100 abutments; MD: minimal thickness crowns cemented on Paradigm MZ100 abutments; ME: minimal thickness crowns cemented on e.max abutments. The 3Shape system was used to scan, design and mill all abutments and crowns with a die space set to 40 mu m. Traditional thickness crowns were designed based on manufacturer guidelines with 1.5 mm occlusal thickness and 1.0 mm margins. Minimal thickness crowns were designed with 0.7 mm occlusal thickness and 0.5 mm margins. MZ100 composite and e.max abutments were selected to simulate dentin and enamel substrates, respectively, based on their elastic-modulus. Variolink Esthetic was used to cement all samples following manufacturer's instructions. A universal testing machine was used to load all specimens to fracture with a 3 mm radius stainless steel hemispherical tip at a crosshead speed 0.5 mm/minute along the longitudinal axis of the abutment with a 1 mm thermoplastic film placed between the loading tip and crown surface. Data was analyzed using ANOVA and Bonferroni post hoc assessment. Fractographic analysis was performed with scanning electron microscopy (SEM). Results: The mean fracture load (standard deviation) was 1499 (241) N for TD; 1228 (287) N for MD; and 1377 (96) N for ME. Statistically significant difference between groups did not exist (p= 0.157, F= 1.995). In groups TD and MD with lowe-modulus abutments, the dispersion of a probability distribution (coefficient of variation: CV) was statistically higher than that of group ME with high e-modulus abutments. SEM illustrated larger micro-fracture dimensions in Group MD than Group ME. Conclusion: Minimal thickness e.max crowns did not demonstrate statistical difference in fracture resistance from traditional thickness crowns. Fracture mechanisms of minimal thickness e.max crowns may be affected by the e-modulus of the substrate. Minimal thickness e.max crowns may be a viable restorative option when supported by high e-modulus materials.
引用
收藏
页码:997 / 1004
页数:8
相关论文
共 27 条
  • [1] Schlichting L.H., Maia H.P., Baratieri L.N., Et al., Novel-design ultra-thin CAD/CAM composite resin and ceramic occlusal veneers for the treatment of severe dental erosion, J Prosthet Dent, 105, pp. 217-225, (2011)
  • [2] Magne P., Schlichting L.H., Maia H.P., Et al., In vitro fatigue resistance of CAD/CAM composite resin and ceramic posterior occlusal veneers, J Prosthet Dent, 104, pp. 149-157, (2010)
  • [3] Edelhoff D., Sorensen J.A., Tooth structure removal associated with various preparation designs for posterior teeth, Int J Periodontics Restor Dent, 22, pp. 241-249, (2002)
  • [4] Magne P., Carvalho A.O., Bruzi G., Et al., Fatigue resistance of ultrathin CAD/CAM complete crowns with a simplified cementation process, J Prosthet Dent, 114, pp. 574-579, (2015)
  • [5] Kim J.H., Lee S.U., Park J.S., Et al., Fracture load of monolithic CAD/CAM lithium disilicate ceramic crowns and veneered zirconia crowns as a posterior implant restoration, Implant Dent, 22, pp. 66-70, (2013)
  • [6] Choi S., Yoon H.I., Park E.J., Load-bearing capacity of various CAD/CAM monolithic molar crowns under recommended occlusal thickness and reduced occlusal thickness conditions, J Adv Prosthodont, 9, pp. 423-431, (2017)
  • [7] Ma L., Guess P.C., Zhang Y., Load-bearing properties of minimal-invasive monolithic lithium disilicate and zirconia occlusal onlays: finite element and theoretical analyses, Dent Mater, 29, pp. 742-751, (2013)
  • [8] Khawi H., Kaizer M., Chughtai A., Et al., Polymer infiltrated ceramic network structures for resistance to fatigue fracture and wear, Dent Mater, 32, pp. 1352-1361, (2017)
  • [9] Kim J.W., Kim J.H., Thompson V.P., Et al., Sliding contact fatigue damage in layered ceramic structures, J Dent Res, 86, pp. 1046-1050, (2007)
  • [10] Kinney J.H., Marshall S.J., Marshall G.W., The mechanical properties of human dentin: a critical review and re-evaluation of the dental literature, Crit Rev Oral Bio Med, 14, pp. 13-29, (2003)