Experimental investigation on erosion resistance of iron boride coatings for steam turbines at high temperatures

被引:24
作者
Cai, Liu-xi [1 ]
Mao, Jing-ru [1 ]
Wang, Shun-sen [1 ]
Di, Juan [1 ]
Feng, Zhen-ping [1 ]
机构
[1] Xi An Jiao Tong Univ, Inst Turbomachinery, Xian 710049, Peoples R China
基金
中国国家自然科学基金;
关键词
Solid particle erosion; thermal spraying coatings; boride coatings; erosion rate; cracks; critical impact angle; LOW-ALLOY STEELS; PARTICULATE FLOWS; TURBOMACHINERY; SUPERALLOYS;
D O I
10.1177/1350650114557105
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this paper, high temperature erosion tests are performed on four typical anti-erosion coatings for high-parameter steam turbine blades using pneumatic accelerated erosion method to simulate the actual erosion environment in power units. With the employment of scanning electron microscope, energy-dispersive X-ray spectroscopy, glancing-angle X-ray diffraction, and Vickers indentation testing techniques, detailed microscopic analysis of samples is conducted to reveal the underlying causes affecting the anti-erosion performance of coatings. Results show that, under the solid particle erosion at high temperature, boride coatings with more compact structure and higher hardness have stronger anti-erosion ability, whose erosion rate is only 30-50% that of HVOF Cr3C2 coatings under the same erosion condition. Boride coatings composed of duplex phase (FeB and Fe2B) have lower anti-erosion damage capability than that of boride coatings composed of single Fe2B phase. Under high-speed large incidence angle impingement, the surface layer of FeB cracks easily and rapidly propagates to the subsurface layer Fe2B phase under the sustained impingement from particles, resulting in the flaking off and failure of coatings. Single Fe2B phase boride coatings have smaller hardness gradient in the depth direction and higher fracture toughness than boride coatings composed of duplex phase, so that exhibit more stable excellent erosion resistance under different erosion parameters. Therefore, single Fe2B phase boride coatings should be used as the preferred wear resistant coating for turbine blades solid particle erosion problem.
引用
收藏
页码:636 / 645
页数:10
相关论文
共 24 条
[11]   Boronizing of cast martensitic chromium nickel stainless steel and its abrasion and cavitation-erosion behaviour [J].
Mann, BS .
WEAR, 1997, 208 (1-2) :125-131
[12]  
Mazur Z., 2002, INT JOINT POW GEN C, P571
[13]   Boronizing and solid particle erosion resistance of 12%Cr heat resistant steel [J].
Miyazaki, Matsuo ;
Ikeda, Kazuaki .
Zairyo/Journal of the Society of Materials Science, Japan, 2002, 51 (04) :412-417
[14]   THE INFLUENCE OF COATING PROCESSES AND PROCESS PARAMETERS ON SURFACE EROSION RESISTANCE AND SUBSTRATE FATIGUE-STRENGTH [J].
QURESHI, JI ;
TABAKOFF, W .
SURFACE & COATINGS TECHNOLOGY, 1988, 36 (1-2) :433-444
[15]  
Qureshi JI, 1987, WEST EL CORP MITS HE
[16]  
Shkol'nik GT, 1970, TEPLOENERGETIKA, V4, P156
[17]   Erosion resistance of superalloys and different coatings exposed to particulate flows at high temperature [J].
Tabakoff, W .
SURFACE & COATINGS TECHNOLOGY, 1999, 120 :542-547
[18]  
Tabakoff W, 1995, SURF COAT TECH, V76, P75, DOI 10.1016/0257-8972(95)02507-3
[19]   HIGH-TEMPERATURE EROSION RESISTANCE OF COATINGS FOR USE IN TURBOMACHINERY [J].
TABAKOFF, W .
WEAR, 1995, 186 (01) :224-229
[20]   Protection of coated superalloys from erosion in turbomachinery and other systems exposed to particulate flows [J].
Tabakoff, W .
WEAR, 1999, 233 :200-208