Study on the interface reaction layer of hydrogen reduction hot-rolled high-strength steel hot-dip galvanizing

被引:3
作者
Liu, Yihao [1 ,2 ,3 ]
Ding, Chengfa [1 ,2 ,3 ]
Li, Jianchao [4 ]
Lu, Rui [1 ,2 ,3 ]
Wu, Guangxin [1 ,2 ,3 ]
Zhang, Jieyu [1 ,2 ,3 ]
机构
[1] Shanghai Univ, Sch Mat Sci & Engn, Shanghai 200444, Peoples R China
[2] Shanghai Univ, State Key Lab Adv Special Steel, Shanghai 200444, Peoples R China
[3] Shanghai Univ, Shanghai Key Lab Adv Ferromet, Shanghai 200444, Peoples R China
[4] Hebei Coll Ind & Technol, Dept Intelligent Mfg, Shijiazhuang 050091, Hebei, Peoples R China
关键词
hydrogen reduction; galvanizing; Fe-Al inhibition layer; hot-rolled high-strength steel; Fe-Zn outburst structure; MICROSTRUCTURE; ACID; CORROSION; IRON; FE; SUBSTRATE; EVOLUTION; COATINGS; SCALE; PHASE;
D O I
10.1088/2053-1591/ac5d7c
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this paper, the instability mechanism of the Fe-Al inhibition layer produced by the interfacial reaction in the Al-containing zinc melts on the hydrogen-reduced steel is studied in detail. The results show that the surface morphology of hydrogen-reduced hot-rolled steel at different temperatures is mainly divided into porous and dense states. Due to the different surface activity of the steel after hydrogen reduction, the reaction degree of the galvanized interface is also significantly different. When the Al content is 0.2 wt%, no Fe-Al inhibition layer is detected at the interface. After that, the influence of Al content on the interface inhibition layer was explored. The research results showed that under the same reduction temperature and inhibition time, the higher the Al content, the more obvious the inhibition layer formed at the interface. Finally, by extending the dipping time, it was confirmed that the Fe-Al inhibition layer had undergone a destabilization and cracking transformation process, that is, the zinc solution permeated the Fe-Al inhibition layer, and the iron interface and the liquid zinc were in direct contact, resulting in the formation of the Fe-Zn outburst structure, which was also aggravated the process of breaking the Fe-Al inhibition layer.
引用
收藏
页数:11
相关论文
共 27 条
[1]   Transformation of Fe-Al phase to Fe-Zn phase on pure iron during galvanizing [J].
Adachi, Y ;
Arai, M .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 254 (1-2) :305-310
[2]   Corrosion of press-hardened galvanized steel [J].
Autengruber, Robert ;
Luckeneder, Gerald ;
Hassel, Achim Walter .
CORROSION SCIENCE, 2012, 63 :12-19
[3]   Studies of the morphology of the Al-Rich interfacial layer formed during the hot dip galvanizing of steel sheet [J].
Baril, E ;
Lespérance, G .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (03) :681-695
[4]   Microstructural Evolution of 11Al-3Mg-Zn Ternary Alloy-Coated Steels During Austenitization Heat Treatment [J].
Chang, Jun-Kai ;
Lin, Chao-Sung .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2017, 48A (08) :3734-3744
[5]   Control of the growth of zinc-iron phases in the hot-dip galvanizing process [J].
Culcasi, JD ;
Seré, PR ;
Elsner, CI ;
Di Sarli, AR .
SURFACE & COATINGS TECHNOLOGY, 1999, 122 (01) :21-23
[6]   Effect of bath aluminum concentration on the galvanizing of hydrogen reduced hot rolled steel without acid pickling [J].
Guan, Chuang ;
Li, Jun ;
Tan, Ning ;
Zhang, Shu-Guang ;
Zhang, Wen-Yue .
SURFACE & COATINGS TECHNOLOGY, 2015, 279 :142-149
[7]   Reduction of oxide scale on hot-rolled steel by hydrogen at low temperature [J].
Guan, Chuang ;
Li, Jun ;
Tan, Ning ;
He, Yong-Quan ;
Zhang, Shu-Guang .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2014, 39 (27) :15116-15124
[8]   Anomalous diffusion of Fe in liquid Al measured by the pulsed laser technique [J].
Isono, N ;
Smith, PM ;
Turnbull, D ;
Aziz, MJ .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1996, 27 (03) :725-730
[9]   Decarburization mechanism during hydrogen reduction descaling of hot-rolled strip steel [J].
Jing, Yu-An ;
Yuan, Yue-Ming ;
Yan, Xiao-Lin ;
Zhang, Lei ;
Sha, Ming-Hong .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2017, 42 (15) :10611-10621
[10]   The evolution of surface morphologies and microstructures during cold rolling after hydrogen reduction [J].
Jing, Yu-an ;
Zang, Xiaoming ;
Shang, Qiuyue ;
Qin, Yi ;
Li, Yinghong ;
Song, Bo .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2015, 219 :303-313