Stress Corrosion Cracking and Localized Corrosion of Carbon Steel in Nitrate Solutions

被引:13
作者
Sridhar, N. [1 ]
Beavers, J. A. [1 ]
Rollins, B. [1 ]
Chawla, S. [1 ]
Evans, K. [1 ]
Li, X. [1 ]
机构
[1] DNV GL, 5777 Frantz Rd, Dublin, OH 43017 USA
关键词
carbon steel; localized corrosion; nitrate; nitrite; radioactive waste storage; repassivation potential; stress corrosion cracking; MILD-STEEL; IRON; REDUCTION; NH4NO3-NH3-H2O; KINETICS; NITRITE; SYSTEM; NANO3; TANKS; FE;
D O I
10.5006/2035
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The stress corrosion cracking (SCC) of carbon steel in nitrate-containing environments has been known for a long time and has become important in managing the integrity of aging underground radioactive waste storage tanks. This paper describes the latest research on the effect of environmental chemistry on localized corrosion and SCC of steel in nitrate-containing solutions, especially as it relates to radioactive waste storage systems. Nitrate is known to be an aggressive species for the localized corrosion and SCC of carbon steel while nitrite, hydroxide, and carbonate are inhibitive species. The role of nitrate and nitrite in localized corrosion and cracking appear to be related to their effects on active dissolution and passivity, rather than on corrosion potential. The long-term corrosion potential is influenced mostly by the pH.
引用
收藏
页码:927 / 942
页数:16
相关论文
共 63 条
[1]   Kinetics of nitrate, nitrite, and Cr(VI) reduction by iron metal [J].
Alowitz, MJ ;
Scherer, MM .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2002, 36 (03) :299-306
[2]  
Anda V., 2010, CORROSION 2010
[3]  
[Anonymous], 2014, G19208 ASTM INT
[4]  
[Anonymous], 2016, CORROSION 2016
[5]  
[Anonymous], 2003, C6186 ASTM INT
[6]  
[Anonymous], 2016, CORROSION 2016
[7]  
[Anonymous], 2016, API 579-1/ASME FFS-1
[8]  
[Anonymous], 2015, E145715 ASTM INT
[9]  
[Anonymous], 2006, G129 ASTM INT
[10]   Corrosion management of the Hanford high-level nuclear waste tanks [J].
Beavers J.A. ;
Sridhar N. ;
Boomer K.D. .
JOM, 2014, 66 (03) :491-502