Infiltration sintering of WCu alloys from copper-coated tungsten composite powders for superior mechanical properties and arc-ablation resistance

被引:63
作者
Chen, Wenge [1 ]
Shi, Yingge [1 ]
Dong, Longlong [1 ]
Wang, Lijian [1 ]
Li, Hanyan [1 ]
Fu, Yongqing [2 ]
机构
[1] Xian Univ Technol, Sch Mat Sci & Engn, Xian 710048, Shaanxi, Peoples R China
[2] Northumbria Univ, Fac Engn & Environm, Newcastle Upon Tyne NE1 8ST, Tyne & Wear, England
基金
中国国家自然科学基金;
关键词
Coated composite powders; Infiltration sintering; WCu alloy; Arc erosion; Breakdown morphology; W-CU COMPOSITES; SURFACE NANO-CRYSTALLIZATION; THERMAL-PROPERTIES; EROSION BEHAVIOR; DENSIFICATION; PARAMETERS; EVOLUTION;
D O I
10.1016/j.jallcom.2017.08.164
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
W70Cu30(W-30 wt.% Cu) alloys were fabricated using cold pressing and infiltration sintering methods from two types of powders, i.e., mixed copper-tungsten (M-Cu-W) powders and our newly developed copper-coated tungsten composite (Cu@W) powders. Microstructure, mechanical and arc-ablation properties of the W70Cu30 alloys were investigated, and the mechanism of enhanced physical/mechanical properties and arc-erosion resistance of the W70Cu30 alloys was discussed. For the W70Cu30 alloys prepared using the Cu@W powders, their physical properties, including hardness, electrical conductivity and relative density were much better than those prepared from the M-Cu-W powders. The W70Cu30 alloys fabricated from the Cu@W powders were free of cracks, and showed homogenous distributions of W and Cu network structures. Whereas for the alloys prepared from the M-Cu-W powders, segregation of Cu was observed and the segregation size was about 40-100 mm. Characterization of arc-erosion morphologies of the W70Cu30 alloys prepared with the Cu@W powders revealed the occurrence of evaporation of Cu phase; whereas that of W70Cu30 alloys prepared with the M-Cu-W powders revealed the occurrence of the sputtering of Cu. After arc breakdown for 200 times, mass loss of alloys made using the mixed powders was twice as much as those made using the coated composite powders. Based on the experimental results and theoretical analysis, an arc breakdown mechanism of the WCu-C alloys using the composite powders was proposed which is attributed to the formation of a homogeneous Cu-Cu network structure to uniformly disperse arc energy and dissipate the generated heat, thus prolonging the service life of the WCu alloy contacts. (c) 2017 Elsevier B.V. All rights reserved.
引用
收藏
页码:196 / 205
页数:10
相关论文
共 32 条
[1]   Synthesis and densification of W-30 wt%Cu composite powders using ammonium meta tungstate and copper nitrate as precursors [J].
Ardestani, M. ;
Arabi, H. ;
Rezaie, H. R. ;
Razavizadeh, H. .
INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2009, 27 (04) :796-800
[2]   Arc erosion behavior of a nanocomposite W-Cu electrical contact material [J].
Chen, W ;
Kang, ZY ;
Shen, HF ;
Ding, BJ .
RARE METALS, 2006, 25 (01) :37-42
[3]  
Chen W., 2003, ELECT MAT, V3, P21
[4]   Investigation and analysis of arc ablation on WCu electrical contact materials [J].
Chen, Wenge ;
Dong, Longlong ;
Zhang, Zhijun ;
Gao, Hongmei .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2016, 27 (06) :5584-5591
[5]  
Costa F.A., 2003, POWDER TECHNOL, V134, P123, DOI DOI 10.1016/50032-5910(03)00123-2
[6]   Investigation on arc erosion behaviors and mechanism of W70Cu30 electrical contact materials adding graphene [J].
Dong, Longlong ;
Chen, Wenge ;
Deng, Nan ;
Song, Jiulong ;
Wang, Jiaojiao .
JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 696 :923-930
[7]   Microstructure and properties characterization of tungsten-copper composite materials doped with graphene [J].
Dong, Longlong ;
Chen, Wenge ;
Zheng, Chenghao ;
Deng, Nan .
JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 695 :1637-1646
[8]   Thermal properties of W-Cu composites manufactured by copper infiltration into tungsten fiber matrix [J].
Duan, Lihui ;
Lin, Wensong ;
Wang, Jieli ;
Yang, Guoliang .
INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2014, 46 :96-100
[9]   Correlations between hardness and atomic bond parameters of pure metals and semi-metals after processing by high-pressure torsion [J].
Edalati, Kaveh ;
Horita, Zenji .
SCRIPTA MATERIALIA, 2011, 64 (02) :161-164
[10]  
Emsley J., 1991, ELEMENTS, P56