Preparation of HBWSL-1 Type Photosensitive Resin for Stereolithography and Study on the Accuracy of Its Fabricated Parts

被引:2
作者
Huang, Biwu [1 ]
Liu, Shimin [1 ]
Chen, Weiqing [1 ]
机构
[1] Nanchang Univ, Sch Mat Sci & Engn, Nanchang, Peoples R China
来源
ADVANCED MATERIALS, PTS 1-4 | 2011年 / 239-242卷
关键词
laser; photosensitive; resin; stereolithography; part; accuracy; THERMAL-DEGRADATION; STRESS-ANALYSIS; SHRINKAGE; PARAMETERS; POLYMERS; KINETICS; CURE;
D O I
10.4028/www.scientific.net/AMR.239-242.3043
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
HBWSL-1 type photosensitive resin for Stereolithography was prepared with bisphenol A type epoxy diacrylate (EA-612), polyethene glycol (200) diacrylate (PEGDA), ethoxylated trimethyolpropane triacrylate (EO(3)TMPTA), cycloaliphatic diepoxide (ERL-4221), polycaprolactone polyol(Polyol-0301), 1-hydroxycyclohexyl phenyl ketone (Irgacure184) and a mixture of triarylsulfonium hexafluoroantimonate salts (UVI-6976). The main parameters of the photosensitive resin were as follows: the penetration depth was 0.15mm, the critical exposure was 16.6mJ/cm(2), the viscosity at 30 degrees C was 215mPa.s, and the density at 30 degrees C was 1.13g/cm(3). With the photosensitive resin as the processing material, cuboid parts and double-cantilever parts were fabricated by using a stereolithography apparatus, and the dimension shrinkage factor and the curl factor were studied. The shrinkage factor was less than 1.00%, and the curl factor was less than 8.00%, which showed that the accuracy of the fabricated parts was high with the photosensitive resin for stereolithography.
引用
收藏
页码:3043 / +
页数:2
相关论文
共 19 条
[1]  
Biwu Huang, 2008, ACTA OPT SINICA, V28, P2354
[2]  
Campanelli S.L., 2003, COMPUT AIDED DESIGN, V136, P146
[3]   Characteristics of photopolymeric material used in rapid prototypes .1. Mechanical properties in the green state [J].
Cheah, CM ;
Nee, AYC ;
Fuh, JYH ;
Lu, L ;
Choo, YS ;
Miyazawa, T .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1997, 67 (1-3) :41-45
[4]   Experimental study of post-build cure of stereolithography polymers for injection molds [J].
Colton, Jonathan ;
Blair, Bryan .
RAPID PROTOTYPING JOURNAL, 1999, 5 (02) :72-81
[5]   Post-cure shrinkage of photo-sensitive material used in laser lithography process [J].
Fuh, JYH ;
Choo, YS ;
Lu, L ;
Nee, AYC ;
Wong, YS ;
Wang, WL ;
Miyazawa, T ;
Ho, SH .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1997, 63 (1-3) :887-891
[6]  
Fuh JYH, 1999, J MATER PROCESS TECH, V90, P211
[7]   Dynamic reverse compensation to increase the accuracy of the rapid prototyping system [J].
Huang, YM ;
Lan, HY .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2005, 167 (2-3) :167-176
[8]   Study of shrinkage strains in a stereolithography cured acrylic photopolyrner resin [J].
Karalekas, D ;
Aggelopoulos, A .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2003, 136 (1-3) :146-150
[9]   On the use of stereolithography built photoelastic models for stress analysis investigations [J].
Karalekas, DE ;
Agelopoulos, A .
MATERIALS & DESIGN, 2006, 27 (02) :100-106
[10]   ORIGIN OF SHRINKAGE, DISTORTION AND FRACTURE OF PHOTOPOLYMERIZED MATERIAL [J].
LU, L ;
FUH, JYH ;
NEE, AYC ;
KANG, ET ;
MIYAZAWA, T ;
CHEAH, CM .
MATERIALS RESEARCH BULLETIN, 1995, 30 (12) :1561-1569