Effects of Different Over - the - Counter Whitening Products on the Microhardness, Surface Roughness, Color and Shear Bond Strength of Enamel

被引:15
|
作者
Yildirim, Esra [1 ]
Vural, Uzay Koc [1 ]
Cakir, Filiz Yalcin [1 ]
Gurgan, Sevil [1 ]
机构
[1] Hacettepe Univ, Sch Dent, Dept Restorat Dent, TR-06100 Ankara, Turkey
关键词
Tooth Whitening; OTC Products; Microhardness; Surface Hardness; Shear Bond Strength; PEROXIDE BLEACHING AGENTS; CARBAMIDE PEROXIDE; EFFICACY; ADHESIVE; SYSTEMS; DENTIN; 10-PERCENT; COMPOSITE; EXPOSURE; LASER;
D O I
10.15644/asc56/2/3
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objective: The purpose of this in vitro study was to evaluate the effects of four over-the-counter (OTC) whitening products on the microhardness, surface roughness, color, shear bond strength (SBS) and surface charecteristics of human enamel compared with a product used for dentist-supervised home whitening. Material and methods: Seventy eight enamel specimens allocated into 6 groups (n=13): 1.Opalescence PF 10% (OP) dentist prescribed home whitening product, 2-Opalescence Go prefilled tray (PT), 3-Opalescence Whitening Toothpaste (W1), 4-Listerine Healthy White whitening mouth rinse (WMR), 5-Cavex Bite&White whitening pen (WP) and 6- no treatment (Con). The microhardness (VHN), surface roughness (Ra) and color of the specimens were measured (Td. The specimens were then subjected to whitening protocols for 14 days (T). followed by artificial saliva storage for 14 days (1 ,). The measurements were repeated at T L and T.. The SBS test was done after the application of 35% phosphoric acid (Scotchbond Universal Etchan0, followed by a universal adhesive (G-Premio Bond) and a micro hybrid/universal resin composite (Essentia) into a Teflon tube attached to the enamel surface (p<0.05). Surface morphologies of the enamel surfaces were examined by SEM. p value was set at 0.05 Results Application of OP, PT and WP decrased the microhardness of enamel specimens (p<0.05) whereas, no significant changes were seen in the microhardness of enamel specimens treated with WT and WMR (p>0.05). Ra values of enamel specimens increased with the application of OP, PT and WT (p<0.05); whereas no changes were observed after the applications of WMR and WP (p>0.05). OP, PT, WMR, and WP changed the color of the enamel(p<0.05). There were not any significant differences among the SBSs of the groups, apart from OP applied enamel specimens. OP showed the least SBS values (p=0.001). SEM observations revealed smooth enamel surfaces. Conclusions: The whitening products affected the microhardness, surface roughness, color of enamel differently. Only OP decreased the SBS of the enamel.
引用
收藏
页码:120 / 131
页数:12
相关论文
共 50 条
  • [11] Effect of different surface treatments and thermocycling on shear bond strength to polyetheretherketone
    Zhou, Li
    Qian, Yuetong
    Gan, Kang
    Liu, Hong
    Liu, Xiuju
    Niu, Deli
    HIGH PERFORMANCE POLYMERS, 2017, 29 (01) : 87 - 93
  • [12] Comparative evaluation of probiotic solutions on surface roughness and microhardness of different restorative materials and enamel
    Karatas, Ozcan
    Delikan, Ebru
    Avunduk, Ayse Tugba Erturk
    JOURNAL OF CLINICAL PEDIATRIC DENTISTRY, 2024, 48 (03) : 107 - 119
  • [14] Shear Bond Strength to Enamel and Flexural Strength of Different Fiber-reinforced Composites
    Juloski, Jelena
    Beloica, Milos
    Goracci, Cecilia
    Chieffi, Nicoletta
    Giovannetti, Agostino
    Vichi, Alessandro
    Vulicevic, Zoran R.
    Ferrari, Marco
    JOURNAL OF ADHESIVE DENTISTRY, 2013, 15 (02) : 123 - 130
  • [15] An In Vitro Comparison of Shear Bond Strength of Zirconia to Enamel Using Different Surface Treatments
    Zandparsa, Roya
    Talua, Nayrouz A.
    Finkelman, Matthew D.
    Schaus, Scott E.
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2014, 23 (02): : 117 - 123
  • [16] Effectiveness of Different Etching Agents on Enamel Surface and Shear Bond Strength: An In Vitro Evaluation
    Jani, Bharvi
    Shah, Alap
    Shankar, Chetan
    Revankar, Siddharth
    Shukla, Hetanshi S.
    Ramalingam, Karthikeyan
    CUREUS JOURNAL OF MEDICAL SCIENCE, 2024, 16 (02)
  • [17] In vitro dentin pretreatment:: Surface roughness and adhesive shear bond strength
    Coli, P
    Alaeddin, S
    Wennerberg, A
    Karlsson, S
    EUROPEAN JOURNAL OF ORAL SCIENCES, 1999, 107 (05) : 400 - 413
  • [18] Demineralization Effects of Hydrogen Heroxide on Bovine Enamel and Relation to Shear Bond Strength of Brackets
    Gonzalez-Lopez, Santiago
    de Medeiros, Carmen Lucia Soares G.
    Defren, Camejo-Aguilar
    Victoria Bolanos-Carmona, Maria
    Sanchez-Sanchez, Purificacion
    Menendez-Nunez, Mario
    JOURNAL OF ADHESIVE DENTISTRY, 2009, 11 (06) : 461 - 467
  • [19] Effect of Different Composite Placement Molds on Resin-Enamel/Dentin Shear Bond Strength
    Ayar, Muhammet Kerim
    Yesilyurt, Cemal
    Yildirim, Tahsin
    JOURNAL OF RESEARCH IN MEDICAL AND DENTAL SCIENCE, 2016, 4 (02): : 141 - 145
  • [20] Effect of enamel laser irradiation at different pulse settings on shear bond strength of orthodontic brackets
    Sagir, Serkan
    Usumez, Aslihan
    Ademci, Ebru
    Usumez, Serdar
    ANGLE ORTHODONTIST, 2013, 83 (06) : 973 - 980