Tritium aging effects on hydrogen permeation through Pd8.5Y0.19Ru alloy membrane

被引:2
作者
Lu Guangda [1 ]
Zhang Guikai [1 ]
Chen Miao [1 ]
Wang Xiaoying [1 ]
机构
[1] China Acad Engn Phys, Mianyang 621900, Peoples R China
关键词
Pd-Y alloy membrane; Hydrogen; Permeation; Tritium aging effect; SEPARATION; SYSTEM; EXPOSURE;
D O I
10.1016/j.fusengdes.2011.04.038
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
Palladium alloy membranes have been widely used as permeator to produce pure tritium from gas mixture or tritiated impurities in tritium technology related to fusion reactor. But long term continuous operation will lead to accumulation of 3 He in alloy, resulting in tritium aging effects. In this work, the changes in protium/deuterium permeation characteristics of Pd8.5Y0.19Ru (at.%) alloy membrane with (3)He concentration of 0.042 (He/M) induced by tritium decay was investigated. In the temperature range 573 K-723 K the permeability of the aged membrane decrease seriously, and the permeation separation factor for H-D mixture increase somewhat. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:2220 / 2222
页数:3
相关论文
共 32 条
  • [31] A comparison between GDP and PDP experiments of hydrogen permeation through 15 μm Pd60-Cu40% membrane thickness in a micro channel plate type reactor
    El-Shafie, Mostafa
    Kambara, Shinji
    Hayakawa, Yukio
    FUSION ENGINEERING AND DESIGN, 2019, 149
  • [32] Effect of Co-existing gases on hydrogen permeation through a Pd82-Ag18/α-Al2O3 membrane during transient start-up
    Budhi, Yogi Wibisono
    Irawan, Hans Kristian
    Fitri, Raihan Annisa
    Wibisono, Tareqh Al Syifa Elgi
    Restiawaty, Elvi
    Miyamoto, Manabu
    Uemiya, Shigeyuki
    HELIYON, 2023, 9 (06)