Thermal-mechanical fatigue behaviour of P92 T-piece and Y-piece pipe

被引:2
作者
Zhang, Wei [1 ]
Wang, Xiaowei [1 ]
Jiang, Yong [1 ]
Gong, Jianming [1 ]
Huang, Xin [1 ]
Weng, Xiaoxiang [1 ]
机构
[1] Nanjing Tech Univ, Sch Mech & Power Engn, Nanjing 211816, Jiangsu, Peoples R China
关键词
Thermal-mechanical fatigue; P92; steel; T-piece and Y-piece pipe; Finite-element model; LOW-CYCLE FATIGUE; THERMOMECHANICAL FATIGUE; DAMAGE MECHANISMS; FAILURE ANALYSIS; STEEL; VISCOPLASTICITY; SIMULATION; MODEL; DEFORMATION;
D O I
10.1080/09603409.2016.1219804
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This paper presents a study on thermal-mechanical fatigue (TMF) behavior of P92 T-piece and Y-piece pipe at the most critical working fluctuations. Pressure and temperature in isothermal, in-phase (IP) and out-of-phase (OP) loading conditions were taken into account. Cyclic plasticity model considering the effect of temperature was used, in which both kinematic hardening variable and isotropic hardening variable are included. All the parameters used in the simulation were obtained from low cycle fatigue (LCF) tests at different temperatures. These parameters have been validated through the comparison of experimental data with the simulated data. Then, finite-element models (FEM) of P92 T-piece and Y-piece pipe were developed to investigate the location of the most critical region at typical thermal-mechanical loading. Simulated results reveal that the most dangerous position occurs at the region where the inner surface of horizontal pipe and branch pipe crossed for both T-piece and Y-piece pipe which is irrelevant to the types of loading. IP loading is the most serious working condition for both T-piece and Y-piece pipe. Comparing with T-piece pipe, Y-piece pipe at IP loading is the most dangerous condition.
引用
收藏
页码:609 / 616
页数:8
相关论文
共 32 条
[21]   Thermomechanical fatigue and damage mechanisms in Sanicro 25 steel [J].
Petras, R. ;
Skorik, V. ;
Polak, J. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 650 :52-62
[22]   Thermomechanical and isothermal fatigue behavior of 347 and 316L austenitic stainless tube and pipe steels [J].
Ramesh, Mageshwaran ;
Leber, Hans J. ;
Janssens, Koenraad G. F. ;
Diener, Markus ;
Spolenak, Ralph .
INTERNATIONAL JOURNAL OF FATIGUE, 2011, 33 (05) :683-691
[23]   Thermal-mechanical fatigue simulation of a P91 steel in a temperature range of 400-600°C [J].
Saad, A. A. ;
Hyde, C. J. ;
Sun, W. ;
Hyde, T. H. .
MATERIALS AT HIGH TEMPERATURES, 2011, 28 (03) :212-218
[24]  
Sun W., 2012, SEG TECHN PROGR, P1
[25]   Strain-gradient modelling of grain size effects on fatigue of CoCr alloy [J].
Sweeney, C. A. ;
O'Brien, B. ;
Dunne, F. P. E. ;
McHugh, P. E. ;
Leen, S. B. .
ACTA MATERIALIA, 2014, 78 :341-353
[26]   T/P23, 24, 911 and 92: New grades for advanced coal-fired power plants-Properties and experience [J].
Vaillant, J. C. ;
Vandenberghe, B. ;
Hahn, B. ;
Heuser, H. ;
Jochum, C. .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2008, 85 (1-2) :38-46
[27]   Characterization of Low Cycle Fatigue of Ferritic-Martensitic P92 Steel: Effect of Temperature [J].
Wang, Xiaowei ;
Jiang, Yong ;
Gong, Jianming ;
Zhao, Yanping ;
Huang, Xin .
STEEL RESEARCH INTERNATIONAL, 2016, 87 (06) :761-771
[28]   Experimental and simulative failure analysis of reformer furnace outlet manifolds serviced in aromatic plant [J].
Wang, Xiaowei ;
Tang, Jianqun ;
Gong, Jianming ;
Geng, Luyang ;
Jiang, Yong ;
Liu, Hao .
ENGINEERING FAILURE ANALYSIS, 2015, 57 :350-362
[29]   Characterization of Low Cycle Fatigue Performance of New Ferritic P92 Steel at High Temperature: Effect of Strain Amplitude [J].
Wang, Xiaowei ;
Gong, Jianming ;
Zhao, Yanping ;
Wang, Yanfei ;
Yu, Minghao .
STEEL RESEARCH INTERNATIONAL, 2015, 86 (09) :1046-1055
[30]  
Xiaowei Wang, 2015, Applied Mechanics and Materials, V750, P41, DOI 10.4028/www.scientific.net/AMM.750.41