Silver content effect on rheological and electrical properties of silver pastes

被引:41
作者
Faddoul, Rita [1 ]
Reverdy-Bruas, Nadege [1 ]
Bourel, Josephine [1 ]
机构
[1] Lab Pulp & Paper Sci & Graph Arts, LGP2, UMR 5518, St Martin Dheres, France
关键词
MICROSTRUCTURE; FABRICATION; DEVICES;
D O I
10.1007/s10854-011-0607-3
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
The novelty of this work is laboratory formulation of environmentally friendly, water-based silver inks adapted for screen printing. The challenge was also to elaborate inks that can withstand temperatures as high as 900 A degrees C. Indeed, when printed on ceramic substrate, they were sintered at these high temperatures. These inks can replace conductive silver pastes present in the market, today, and containing irritant solvents such as terpineol and other aromatic solvents. Besides, screen printing is considered as an additive technique, thus allowing reducing wastes. Furthermore, only with 72.5% silver, considered as low content compared to commercial inks (a parts per thousand yen75%), prepared inks presented good electrical resistivity, 23 na"broken vertical bar m, close to that of bulk silver resistivity, 16 na"broken vertical bar m. Formulation of silver inks with spherical particles, 2-3 mu m mean diameter, was performed. The aim of the study was to determine silver content effect on pastes rheological behaviour, lines properties (width, thickness and roughness) and electrical properties. Therefore, rheological behaviour of inks was studied; in particular, Casson and Bingham models were applied in order to determine the yield stress. Viscosity evolution as a function of shear rate was also determined. Besides, the thixotropic behaviour of inks was highlighted. Inks were then screen printed on alumina sintered substrates and cured at different temperatures during 15 min. Topography measurements were performed. Line resistivity as small as 35 na"broken vertical bar m was measured on cured lines. These inks, printed on ceramic tapes, can be used to print microwave transmission lines, for which resistivities lower than 1 ma"broken vertical bar m are requested.
引用
收藏
页码:1415 / 1426
页数:12
相关论文
共 26 条
[1]  
Buzby D., 2011, HEREAUS WHITE PAPERS
[2]   Conductive Adhesives From Low-VOC Silver Inks for Advanced Microelectronics Applications [J].
Datta, Samali ;
Keller, Kristen ;
Schulz, Douglas L. ;
Webster, Dean C. .
IEEE TRANSACTIONS ON COMPONENTS PACKAGING AND MANUFACTURING TECHNOLOGY, 2011, 1 (01) :69-75
[3]  
Goodwin JW, 2008, RHEOLOGY FOR CHEMISTS: AN INTRODUCTION, P1
[4]   Effect of dispersibility of silver powders in conductive paste on microstructure of screen-printed front contacts and electrical performance of crystalline silicon solar cells [J].
Guo, Guiquan ;
Gan, Weiping ;
Xiang, Feng ;
Zhang, Jinling ;
Zhou, Hua ;
Liu, Huan ;
Luo, Jian .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2011, 22 (05) :527-530
[5]   In-house development of co-fireable thick film silver conductor for LTCC applications [J].
Jagtap, Shweta ;
Deshpande, Varsha ;
Rane, Vivek ;
Rane, Sunit ;
Phatak, Girish ;
Amalnerkar, Dinesh .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2008, 19 (06) :522-527
[6]   Fabrication and application of a full wafer size micro/nanostencil for multiple length-scale surface patterning [J].
Kim, GM ;
van den Boogaart, MAF ;
Brugger, J .
MICROELECTRONIC ENGINEERING, 2003, 67-8 :609-614
[7]  
Leach R.H., 1993, The Printing Ink Manual - Google Books
[8]   Effect of surface energies on screen printing resolution [J].
Liang, TX ;
Sun, WZ ;
Wang, LD ;
Wang, YH ;
Li, HD .
IEEE TRANSACTIONS ON COMPONENTS PACKAGING AND MANUFACTURING TECHNOLOGY PART B-ADVANCED PACKAGING, 1996, 19 (02) :423-426
[9]  
Maeder T., 2008, INTRO PATES ENCRES S
[10]   The characterization of electrically conductive silver ink patterns on flexible substrates [J].
Merilampi, S. ;
Laine-Ma, T. ;
Ruuskanen, P. .
MICROELECTRONICS RELIABILITY, 2009, 49 (07) :782-790