Use of glass waste as mineral filler in hot mix asphalt

被引:32
作者
Saltan, Mehmet [1 ]
Oksuz, Betul [1 ]
Uz, Volkan Emre [2 ]
机构
[1] Suleyman Demirel Univ, Dept Civil Engn, Fac Engn, TR-32260 Isparta, Turkey
[2] Univ Sci & Technol, Dept Civil Engn, Fac Engn & Nat Sci, TR-01180 Adana, Turkey
关键词
glass waste; hot mix asphalt; Marshall stability test; mineral filler; CONCRETE; MIXTURE;
D O I
10.1515/secm-2013-0135
中图分类号
TB33 [复合材料];
学科分类号
摘要
The use of resources is increasing due to continuous increase in world population and rapid industrialization, while natural resources are being exhausted day by day. Usage of waste materials or by-products in highway construction has substantial environmental and economic benefits. In this study, the usage of cullet and waste glass bottle dust as mineral filler material in hot mix asphalt as an alternate to traditional crushed stone dust was investigated. Optimum bitumen content was determined by the Marshall mix design method by using six different bitumen contents (4.0%, 4.5%, 5.0%, 5.5%, 6.0%, and 6.5%). With the optimum bitumen content, three different mineral filler types (cullet, glass bottle waste, and stone dust) and six different filler ratios (4%, 5%, 6%, 7%, 8%, and 9%) were used to prepare asphalt mixture samples. Samples were performed using the Marshall stability test, and the results were compared. It is concluded that cullet and glass bottle waste can be used in asphalt mixtures as a mineral filler alternate to crushed stone dust if the economic and environmental factors favor it.
引用
收藏
页码:271 / 277
页数:7
相关论文
共 22 条
  • [1] Acar S, 1998, 2 NAT ASPH S, P95
  • [2] Ahmed H. Y., 2006, J. Ass. Univ. Bull. Environ, V9, P51
  • [3] Ahmedzade P, 2008, IMO TECH J, V19, P4539
  • [4] [Anonymous], D155989 ASTM
  • [5] [Anonymous], 1992, C854 ASTM
  • [6] [Anonymous], 2003, D597 ASTM
  • [7] ASTM, 1992, C127 ASTM
  • [8] ASTM, 2003, D7003 ASTM
  • [9] ASTM, 1992, C128 ASTM
  • [10] Caglar GA, 2007, THESIS ISTANBUL TECH