Facile preparation of a cellulose derived carbon/BN composite aerogel for superior electromagnetic wave absorption

被引:41
作者
Wang, Dedong [1 ]
Zhang, Minyue [1 ]
Guo, Yan [1 ]
Bai, Tiantian [1 ]
Liu, Hu [1 ]
Liu, Chuntai [1 ]
Shen, Changyu [1 ]
机构
[1] Zhengzhou Univ, Natl Engn Res Ctr Adv Polymer Proc Technol, Key Lab Mat Proc & Mold, Minist Educ, Zhengzhou 450002, Henan, Peoples R China
基金
中国国家自然科学基金;
关键词
MICROWAVE; CONSTRUCTION; GRAPHENE; BORON; FABRICATION; PARTICLES; NANOWIRES;
D O I
10.1039/d2tc00205a
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Carbon-based aerogels have been widely accepted to be a type of promising electromagnetic microwave (EMW) absorber due to their merits of low density, high specific surface area, and a three-dimensional porous structure, but the contradiction between their strong dielectric loss capacity and poor impedance matching often results in a weak EMW absorption capacity. In this work, a cellulose derived carbon/BN composite aerogel (CCA/BN) was prepared by a simple freeze-drying and high-temperature pyrolysis process. Here, both the BN loading and pyrolysis temperature could directly affect the dielectric loss capacity of the prepared CCA/BN. Specifically, the abundant interfaces between BN and the carbon matrix and the pyrolysis-generated carbon defects contributed to the polarization loss, and the BN loading and pyrolysis temperature dependent electrical conductivity affected the conduction loss. More importantly, good impedance matching was achieved by adjusting the BN loading and pyrolysis temperature, enabling as much EMW as possible to enter the absorber to be dissipated. What's more, the porous structure also contributed to enhanced EMW absorption efficiency through multiple reflection/scattering inside the material. As a result, CCA/BN with 10 wt% BN and a pyrolysis temperature of 680 degrees C (CCA/BN10-680) exhibited a superior EMW absorption performance with a minimum RL value (RLmin) of -49.2 dB at 11.28 GHz and 3.75 mm thickness and a maximum effective absorption bandwidth (EAB(max)) of 8.16 GHz (9.68-17.84 GHz) at 3.45 mm thickness. This study provides a reliable reference for preparing a highly efficient biomass carbon based EMW absorber.
引用
收藏
页码:5311 / 5320
页数:10
相关论文
共 62 条
[61]   Silica-Modified Ordered Mesoporous Carbon for Optimized Impedance-Matching Characteristic Enabling Lightweight and Effective Microwave Absorbers [J].
Zhou, Panpan ;
Zhang, Jing ;
Zhu, Hongli ;
Wang, Lixi ;
Wang, Xiaokang ;
Song, Zhi ;
Zhang, Qitu ;
Yu, Mingxun ;
Liu, Zhihao ;
Xu, Tong ;
Feng, Wanxun ;
Feng, Xia .
ACS APPLIED MATERIALS & INTERFACES, 2020, 12 (20) :23252-23260
[62]   A reconsideration of the relationship between the crystallite size La of carbons determined by X-ray diffraction and Raman spectroscopy [J].
Zickler, Gerald A. ;
Smarsly, Bernd ;
Gierlinger, Notburga ;
Peterlik, Herwig ;
Paris, Oskar .
CARBON, 2006, 44 (15) :3239-3246