Effect of hot water and heat treatment on the apatite-forming ability of titania films formed on titanium metal via anodic oxidation in acetic acid solutions

被引:37
作者
Cui, Xinyu [2 ]
Kim, Hyun-Min [3 ]
Kawashita, Masakazu [1 ]
Wang, Longbao [2 ]
Xiong, Tianying [2 ]
Kokubo, Tadashi [4 ]
Nakamura, Takashi [5 ]
机构
[1] Tohoku Univ, Ctr Res Strategy & Support, Aoba Ku, Sendai, Miyagi 9808579, Japan
[2] Chinese Acad Sci, Inst Met Res, Shenyang 110016, Peoples R China
[3] Yonsei Univ, Sch Adv Mat Engn, Dept Ceram Engn, Seoul 120749, South Korea
[4] Chubu Univ, Coll Life & Hlth Sci, Dept Biomed Sci, Kasugai, Aichi 4878501, Japan
[5] Kyoto Univ, Grad Sch Med, Dept Orthoped Surg, Kyoto 6158507, Japan
关键词
D O I
10.1007/s10856-007-3314-0
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Titanium and its alloys have been widely used for orthopedic implants because of their good biocompatibility. We have previously shown that the crystalline titania layers formed on the surface of titanium metal via anodic oxidation can induce apatite formation in simulated body fluid, whereas amorphous titania layers do not possess apatite-forming ability. In this study, hot water and heat treatments were applied to transform the titania layers from an amorphous structure into a crystalline structure after titanium metal had been anodized in acetic acid solution. The apatite-forming ability of titania layers subjected to the above treatments in simulated body fluid was investigated. The XRD and SEM results indicated hot water and/or heat treatment could greatly transform the crystal structure of titania layers from an amorphous structure into anatase, or a mixture of anatase and rutile. The abundance of Ti-OH groups formed by hot water treatment could contribute to apatite formation on the surface of titanium metals, and subsequent heat treatment would enhance the bond strength between the apatite layers and the titanium substrates. Thus, bioactive titanium metals could be prepared via anodic oxidation and subsequent hot water and heat treatment that would be suitable for applications under load-bearing conditions.
引用
收藏
页码:1767 / 1773
页数:7
相关论文
共 46 条
[1]  
Aoki H., 1977, J. Dent. Outlook, V49, P567
[2]   PLASMA SPRAYED COATINGS OF HYDROXYLAPATITE [J].
DEGROOT, K ;
GEESINK, R ;
KLEIN, CPAT ;
SEREKIAN, P .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1987, 21 (12) :1375-1381
[3]  
Hench L.L., 1971, Journal of Biomedical Materials Research Symposium, V36, P117, DOI DOI 10.1002/JBM.820050611
[4]   FORMATION AND CHARACTERIZATION OF ANODIC TITANIUM-OXIDE FILMS CONTAINING CA AND P [J].
ISHIZAWA, H ;
OGINO, M .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1995, 29 (01) :65-72
[5]  
JARCHO M, 1977, J BIOENG, V1, P79
[6]   Apatite formation on CaO-free polydimethylsiloxane (PDMS)-TiO2 hybrids [J].
Kamitakahara, M ;
Kawashita, M ;
Miyata, N ;
Kokubo, T ;
Nakamura, T .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 2003, 14 (12) :1067-1072
[7]   Apatite-forming ability and mechanical properties of CaO-free poly(tetramethylene oxide) (PTMO)-TiO2 hybrids treated with hot water [J].
Kamitakahara, M ;
Kawashita, M ;
Miyata, N ;
Kokubo, T ;
Nakamura, T .
BIOMATERIALS, 2003, 24 (08) :1357-1363
[8]   Bonelike apatite formation on anodically oxidized titanium metal in simulated body fluid [J].
Kawashita, M ;
Cui, XY ;
Kim, HM ;
Kokubo, T ;
Nakamura, T .
BIOCERAMICS, VOL 16, 2004, 254-2 :459-462
[9]   Novel bioactive materials with different mechanical properties [J].
Kokubo, T ;
Kim, HM ;
Kawashita, M .
BIOMATERIALS, 2003, 24 (13) :2161-2175
[10]   BIOACTIVE GLASS-CERAMICS - PROPERTIES AND APPLICATIONS [J].
KOKUBO, T .
BIOMATERIALS, 1991, 12 (02) :155-163