Effect of Initial Deflection of Diamond Wire on Thickness Variation of Sapphire Wafer in Multi-Wire Saw

被引:42
作者
Kim, Doyeon [1 ,2 ]
Kim, Hyoungjae [1 ]
Lee, Sangjik [1 ]
Jeong, Haedo [2 ]
机构
[1] Korea Inst Ind Technol, Busan 618230, South Korea
[2] Pusan Natl Univ, Grad Sch Mech Engn, Busan 609836, South Korea
关键词
Diamond wire; Multi wire saw; Sapphire wafer; Total thickness variation; Wire deflection;
D O I
10.1007/s40684-015-0015-x
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Sapphire wafers are widely used as substrates for fabricating gallium nitride light-emitting diodes. The quality of light-emitting diodes depends on the total thickness variation and BOW of the wafers. The multi-wire saw process is critical in determining post-processing times for steps such as diamond mechanical polishing and chemical mechanical polishing. In particular, thickness variation is affected by wear of diamond wires, which in turn is controlled by cutting conditions including wire speed, feed rate, initial contact condition between ingot and wire, and new wire consumption. Thickness variation shows a marked change from the initial to final feeding location during the multi-wire sawing process. A wire is not worn when it is initially contacted by an ingot. Hence, the initial kerf loss is greater than the kerf loss at the final feeding location. This study focused on minimizing the thickness variation between the initial and final contact points of the wafer: Experiments were conducted with different initial wire deflection conditions. The experimental results showed that increasing the wire deflection increased the cutting load, which in turn caused severe wear of the wire. Consequently, the thickness variation of the wafer in the multi-wire sawing process was controlled by adjusting the wire deflection.
引用
收藏
页码:117 / 121
页数:5
相关论文
共 11 条
[1]   Development of a high-speed manufacturing method for electroplated diamond wire tools [J].
Chiba, Y ;
Tani, Y ;
Enomoto, T ;
Sato, H .
CIRP ANNALS-MANUFACTURING TECHNOLOGY, 2003, 52 (01) :281-284
[2]   Generation of diamond wire sliced wafer surface based on the distribution of diamond grits [J].
Chung, Chunhui ;
Le Van Nhat .
INTERNATIONAL JOURNAL OF PRECISION ENGINEERING AND MANUFACTURING, 2014, 15 (05) :789-796
[3]   Fixed abrasive diamond wire machining - part I: process monitoring and wire tension force [J].
Clark, WI ;
Shih, AJ ;
Hardin, CW ;
Lemaster, RL ;
McSpadden, SB .
INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2003, 43 (05) :523-532
[4]   Multi-wire sawing of sapphire crystals with reciprocating motion of electroplated diamond wires [J].
Kim, Hyoungjae ;
Kim, Doyeon ;
Kim, Chulmin ;
Jeong, Haedo .
CIRP ANNALS-MANUFACTURING TECHNOLOGY, 2013, 62 (01) :335-338
[5]  
LEDinside, SAPPH SUBSTR DOM LED
[6]   Effect of wafer size on material removal rate and its distribution in chemical mechanical polishing of silicon dioxide film [J].
Lee, Hyunseop ;
Park, Yeongbong ;
Lee, Sangjik ;
Jeong, Haedo .
JOURNAL OF MECHANICAL SCIENCE AND TECHNOLOGY, 2013, 27 (10) :2911-2916
[7]  
Lee S., 2013, P ASIAN SOC PRECISIO
[8]   Modification of Archard's equation by taking account of elastic/pseudoelastic properties of materials [J].
Liu, R ;
Li, DY .
WEAR, 2001, 251 :956-964
[9]  
Ludema K.C., 1996, Friction, Wear, Lubrication: A Textbook in Tribology
[10]  
Suh N.P., 1986, TRIBOPHYSICS