Fatigue properties of a biomedical 316L steel processed by surface mechanical attrition

被引:10
作者
Sun, Z. [1 ]
Chemkhi, M. [1 ]
Kanoute, P. [1 ]
Retraint, D. [1 ]
机构
[1] Univ Technol Troyes, LASMIS, CNRS, ICD,P2MN,UMR 6281, Troyes, France
来源
6TH INTERNATIONAL CONFERENCE ON NANOMATERIALS BY SEVERE PLASTIC DEFORMATION (NANOSPD6) | 2014年 / 63卷
关键词
LOW-CYCLE FATIGUE; AUSTENITE STABILITY; STAINLESS-STEEL; BEHAVIOR; TRANSFORMATION; LIVES; LAYER;
D O I
10.1088/1757-899X/63/1/012021
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This work deals with the influence of surface mechanical attrition treatment ( SMAT) on fatigue properties of a medical grade 316L stainless steel. Metallurgical parameters governed by SMAT such as micro-hardness and nanocrystalline layer are characterized using different techniques. Low cycle fatigue tests are performed to investigate the fatigue properties of untreated and SMAT-processed samples. The results show that the stress amplitude of SMAT-processed samples with two different treatment intensities is significantly enhanced compared to untreated samples, while the fatigue strength represented by the number of cycles to failure is not improved in the investigated strain range. The enhancement in the stress amplitude of treated samples can be attributed to the influence of the SMAT affected layer.
引用
收藏
页数:10
相关论文
共 23 条
[1]   Nanosized Controlled Surface Pretreatment of Biometallic Alloy 316L Stainless Steel [J].
Abdel-Fattah, Tarek M. ;
Loftis, Derek ;
Mahapatro, Anil .
JOURNAL OF BIOMEDICAL NANOTECHNOLOGY, 2011, 7 (06) :794-800
[2]   Effect of grain size on austenite stability and room temperature low cycle fatigue behaviour of solution annealed AISI 316LN austenitic stainless steel [J].
Basu, K. ;
Das, M. ;
Bhattacharjee, D. ;
Chakraborti, P. C. .
MATERIALS SCIENCE AND TECHNOLOGY, 2007, 23 (11) :1278-1284
[3]   Evaluation of the effect of three surface treatments on the biocompatibility of 316L stainless steel using human differentiated cells [J].
Bordji, K ;
Jouzeau, EY ;
Mainard, D ;
Payan, E ;
Delagoutte, JP ;
Netter, P .
BIOMATERIALS, 1996, 17 (05) :491-500
[4]   The effect of surface mechanical attrition treatment on low temperature plasma nitriding of an austenitic stainless steel [J].
Chemkhi, M. ;
Retraint, D. ;
Roos, A. ;
Garnier, C. ;
Waltz, L. ;
Demangel, C. ;
Proust, G. .
SURFACE & COATINGS TECHNOLOGY, 2013, 221 :191-195
[5]   Analysis of fatigue resistance improvements via surface severe plastic deformation [J].
Dai, K. ;
Shaw, L. .
INTERNATIONAL JOURNAL OF FATIGUE, 2008, 30 (08) :1398-1408
[6]   Effect of austenite stability on the low cycle fatigue behavior and microstructure of high alloyed metastable austenitic cast TRIP-steels [J].
Glage, A. ;
Weidner, A. ;
Biermann, H. .
FATIGUE 2010, 2010, 2 (01) :2085-2094
[7]  
HALFORD GR, 1966, J MATER, V1, P3
[8]  
Jeon YC, 2008, MATER SCI FORUM, V580-582, P597, DOI 10.4028/0-87849-383-2.597
[9]   Monitoring fatigue degradation in austenitic stainless steels [J].
Kalkhof, D ;
Grosse, M ;
Niffenegger, M ;
Leber, HJ .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2004, 27 (07) :595-607
[10]   FATIGUE PROPERTIES OF SPECIMENS SIMILAR TO COMPONENTS DEEP ROLLED UNDER OPTIMIZED CONDITIONS [J].
KLOOS, KH ;
FUCHSBAUER, B ;
ADELMANN, J .
INTERNATIONAL JOURNAL OF FATIGUE, 1987, 9 (01) :35-42