Bond Strength and Interfacial Micromorphology of Etch-and-Rinse and Self-Adhesive Resin Cements to Dentin

被引:47
|
作者
Vaz, Ricardo Rodrigues [2 ]
Di Hipolito, Vinicius [1 ]
D'Alpino, Paulo Henrique [1 ]
de Goes, Mario Fernando [3 ]
机构
[1] Anhanguera Uniban Univ, Sch Dent, Biomat Res Grp, BR-02071013 Sao Paulo, Brazil
[2] Univ Fed Minas Gerais, Sch Dent, Dept Restorat Dent, Belo Horizonte, MG, Brazil
[3] State Univ Campinas UNICAMP, Dept Restorat Dent, Piracicaba Sch Dent, Piracicaba, Brazil
来源
JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY | 2012年 / 21卷 / 02期
关键词
Adhesion strategies; indirect restoration; micromorphology; bonding durability; LUTING CEMENTS; COMPOSITE; SYSTEMS; NANOLEAKAGE; ENAMEL; TISSUE; AGENTS;
D O I
10.1111/j.1532-849X.2011.00794.x
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: To evaluate the microtensile bond strength and interfacial micromorphology of indirect composite restorations to dentin using three commercial resin cements after 24 hours and 30 days of water storage. Materials and Methods: The medium dentin of third human molars was exposed (N = 30, n = 10 per group). Three commercial resin cements were used to cement indirect resin composite restorations to dentin: the auto-cured C& B Cement/All Bond 2, the dual-cured RelyX ARC/Adper Single Bond 2, and the self-adhesive dualcured RelyX Unicem. Teeth were sectioned after water storage at 37 degrees C (24 hours and 30 days) to obtain beams with a bonded area of 0.8 mm(2). The specimens were tested in a universal testing machine at a 0.5 mm/min crosshead speed. Scanning electron microscopic fractographic and interfacial micromorphology analyses were performed. Data were analyzed using two-way ANOVA and Tukey's test (alpha = 0.05). Results: Mean bond strength (MPa) after 24 hours: C& B Cement 19.5 +/- 3.8, RelyX ARC 40.8 +/- 9.4, RelyX Unicem 31.3 +/- 7.4; after 30 days: C& B Cement 24.5 +/- 5.1, RelyX ARC 44.2 +/- 8.5, RelyX Unicem 28.3 +/- 7.1. The mean bond strengths of both dual-cure cements were significantly higher than that obtained with C& B Cement after 24 hours. A significant increase in the bond strength of C& B Cement was verified after 30 days, reaching values statistically equivalent to those produced by RelyX Unicem and RelyX ARC. The self-adhesive cement preserved the same level of bond strength after 30 days. Fractographic analysis revealed a prevalence of cohesive fractures in the hybrid layer for C& B Cement, mixed (cohesive in the cement, hybrid layer, and adhesive) for RelyX ARC, and cohesive in the cement for RelyX Unicem. No distinguishable hybrid layer or resin tags were observed in the interaction of RelyX Unicem with dentin. Conclusions: The particular interaction of each cement with dentin results in specific bond strength and failure patterns that varied among groups in both evaluation times. Even though the self-adhesive cement tested exhibited no authentic hybrid layer, it was able to promote reliable adhesion with the underlying dentin.
引用
收藏
页码:101 / 111
页数:11
相关论文
共 50 条
  • [1] Shear bond strength of self-adhesive resins compared to resin cements with etch and rinse adhesives to enamel and dentin in vitro
    Luehrs, A.-K.
    Guhr, S.
    Guenay, H.
    Geurtsen, W.
    CLINICAL ORAL INVESTIGATIONS, 2010, 14 (02) : 193 - 199
  • [2] Effectiveness of dentin pre-treatment on bond strength of two self-adhesive resin cements compared to an etch-and-rinse system: an in vitro study
    Hammal, Milad
    Chlup, Zdenek
    Ingr, Tomas
    Stanek, Jan
    Mounajjed, Radek
    PEERJ, 2021, 9
  • [3] Effect of air abrasion and thermocycling on resin adaptation and shear bond strength to dentin for an etch-and-rinse and self-etch resin adhesive
    Freeman, Rebecca
    Varanasi, Srinivas
    Meyers, Ian A.
    Symons, Anne L.
    DENTAL MATERIALS JOURNAL, 2012, 31 (02) : 180 - 188
  • [4] Microshear bond strength and interfacial morphology of etch-and-rinse and self-etch adhesive systems to superficial and deep dentin
    Yousry, Mai Mahmoud
    ElNaga, Albeer Abo
    Hafez, Randa M.
    El-Badrawy, Wafa
    QUINTESSENCE INTERNATIONAL, 2011, 42 (09): : E96 - E106
  • [5] Shear bond strength of self-adhesive resins compared to resin cements with etch and rinse adhesives to enamel and dentin in vitro
    A.-K. Lührs
    S. Guhr
    H. Günay
    W. Geurtsen
    Clinical Oral Investigations, 2010, 14 : 193 - 199
  • [6] Influence of resin coating on bond strength of self-adhesive resin cements to dentin
    Giannini, Marcelo
    Takagaki, Tomohiro
    Bacelar-Sa, Renata
    Vermelho, Paulo Moreira
    Ambrosano, Glaucia Maria Bovi
    Sadr, Alireza
    Nikaido, Toru
    Tagami, Junji
    DENTAL MATERIALS JOURNAL, 2015, 34 (06) : 822 - 827
  • [7] Effect of Curing Mode on Bond Strength of Self-Adhesive Resin Luting Cements to Dentin
    Aguiar, T. R.
    Di Francescantonio, M.
    Ambrosano, G. M. B.
    Giannini, M.
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2010, 93B (01) : 122 - 127
  • [8] Bond Strength of an Etch-and-Rinse Adhesive to KrF Excimer Laser-Treated Dentin
    Eugenio, Sonia
    Osorio, Raquel
    Sivakumar, Manickam
    Vilar, Rui
    Monticelli, Francesca
    Toledano, Manuel
    PHOTOMEDICINE AND LASER SURGERY, 2010, 28 (01) : 97 - 102
  • [9] Push-out bond strength of CAD/CAM-ceramic luted to dentin with self-adhesive resin cements
    Flury, Simon
    Lussi, Adrian
    Peutzfeldt, Anne
    Zimmerli, Brigitte
    DENTAL MATERIALS, 2010, 26 (09) : 855 - 863
  • [10] Influence of surface energy parameters of dental self-adhesive resin cements on bond strength to dentin