Tribological properties of HVOF sprayed WC-Cr3C2-Ni coating

被引:17
作者
Goyal, Ayush Kumar [1 ]
Sapate, S. G. [1 ]
Mehar, S. [1 ,2 ]
Vashishtha, N. [1 ,3 ]
Bagde, P. [2 ]
Rathod, A. [3 ]
机构
[1] VNIT, Dept Met & Mat Engn, South Ambazari Rd, Nagpur 440010, Maharashtra, India
[2] GCOE, Dept Mech Engn, Chandrapur 442403, India
[3] NIT Warangal, Dept Met & Mat Engn, Warangal 506004, Andhra Pradesh, India
关键词
cermet; coatings; abrasive wear; friction; brittle fracture; ABRASIVE WEAR BEHAVIOR; WC-CO; HEAT-TREATMENT; PARTICLE-SIZE; SLIDING WEAR; WC-12CO; MICROSTRUCTURE; FRICTION; MECHANISMS;
D O I
10.1088/2053-1591/ab3946
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The deposition of WC-Cr3C2-Ni coating was done by High velocity Oxy Fuel (HVOF) technique. Microstructural and mechanical properties of coating were measured. Friction and abrasive wear response was evaluated with varying loads and sliding velocities. An increase of 1.6-2 times in friction coefficient (COF) was noted with rise in load and COF reduced by around 15%-20% for rise in sliding velocity. Abrasion wear rate reduced by around 2 times with rise in sliding velocity. The decrease in wear rate and COF at higher sliding velocity was due to lubricating properties of tribo oxides formed due to frictional heating. The composition of tribo oxides on worn surface as indicated by XRD analysis revealed different oxides of tungsten, chromium and nickel such as WO3, W3O8, NiO2, NiWO4, NiCr2O4 and CrO2. With increasing load, carbide pull out, delamination cracking, carbide fracture and inter splat fracture were the dominating mechanisms of material removal, whereas with increasing velocity tribo oxidation leading to oxidative wear was dominant wear mechanism.
引用
收藏
页数:12
相关论文
共 25 条
[1]   Abrasive wear behavior of detonation sprayed WC-12Co coatings: Influence of decarburization and abrasive characteristics [J].
Babu, P. Suresh ;
Basu, Bikramjit ;
Sundararajan, G. .
WEAR, 2010, 268 (11-12) :1387-1399
[2]   Friction and wear behaviour of plasma sprayed Cr2O3-TiO2 coating [J].
Bagde, Pranay ;
Sapate, S. G. ;
Khatirkar, R. K. ;
Vashishtha, Nitesh ;
Tailor, Satish .
MATERIALS RESEARCH EXPRESS, 2018, 5 (02)
[3]  
Blau P., 1992, Friction, lubrication and Wear Technologies, V18th, DOI DOI 10.31399/ASM.HB.V18.9781627081924
[4]   Processing optimization, surface properties and wear behavior of HVOF spraying WC-CrC-Ni coating [J].
Fang, W. ;
Cho, T. Y. ;
Yoon, J. H. ;
Song, K. O. ;
Hur, S. K. ;
Youn, S. J. ;
Chun, H. G. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2009, 209 (07) :3561-3567
[5]   Tribological behaviour at various temperatures of WC-Co coatings prepared using different thermal spraying techniques [J].
Geng, Zhe ;
Hou, Sihan ;
Shi, Gaolian ;
Duan, Deli ;
Li, Shu .
TRIBOLOGY INTERNATIONAL, 2016, 104 :36-44
[6]   Behavior of HVOF WC-10Co4Cr Coatings with Different Carbide Size in Fine and Coarse Particle Abrasion [J].
Ghabchi, Arash ;
Varis, Tommi ;
Turunen, Erja ;
Suhonen, Tomi ;
Liu, Xuwen ;
Hannula, S. -P. .
JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2010, 19 (1-2) :368-377
[7]   Influence of WC carbide particle size on the microstructure and abrasive wear behavior of WC-10Co-4Cr coatings for aircraft landing gear [J].
Gong, Taimin ;
Yao, Pingping ;
Zuo, Xiaoting ;
Zhang, Zhongyi ;
Xiao, Yelong ;
Zhao, Lin ;
Zhou, Haibin ;
Deng, Minwen ;
Wang, Qi ;
Zhong, Aiwen .
WEAR, 2016, 362 :135-145
[8]   Analytical characterization of the corrosion mechanisms of WC-Co by electrochemical methods and inductively coupled plasma mass spectroscopy [J].
Hochstrasser-Kurz, S. ;
Mueller, Y. ;
Latkoczy, C. ;
Virtanen, S. ;
Schmutz, P. .
CORROSION SCIENCE, 2007, 49 (04) :2002-2020
[9]  
Hutchings I.M., 1992, FRICTION WEAR ENG MA
[10]   Sliding wear properties of HVOF sprayed WC-20%Cr3C2-7%Ni cermet coatings [J].
Ishikawa, Yasunari ;
Kuroda, Seiji ;
Kawakita, Jin ;
Sakamoto, Yukihiro ;
Takaya, Matsufumi .
SURFACE & COATINGS TECHNOLOGY, 2007, 201 (08) :4718-4727