Characterization and elevated-temperature tribological performance of AC-HVAF-sprayed Fe-based amorphous coating

被引:44
作者
Liang, Dandan [1 ,2 ]
Ma, Jiang [1 ]
Cai, Yuanfei [3 ]
Liu, Xiaodi [1 ]
Xie, Shunde [1 ]
Wei, Xianshun [3 ]
Xu, Gang [1 ]
Shen, Jun [1 ]
机构
[1] Shenzhen Univ, Coll Mechatron & Control Engn, Shenzhen 518060, Guangdong, Peoples R China
[2] Shenzhen Univ, Coll Optoelect Engn, Key Lab Optoelect Devices & Syst, Minist Educ & Guangdong Prov, Shenzhen 518060, Guangdong, Peoples R China
[3] Tongji Univ, Coll Mat Sci & Engn, Shanghai 201804, Peoples R China
基金
中国国家自然科学基金;
关键词
AC-HVAF; Amorphous coating; Elevated temperature; Hardness; Oxidation; Wear mechanism; BULK METALLIC GLASSES; SLIDING WEAR BEHAVIOR; EROSION-CORROSION; HARDNESS; MICROSTRUCTURE; RESISTANCE; FABRICATION; MOLYBDENUM; PARTICLES; COMPOSITE;
D O I
10.1016/j.surfcoat.2020.125535
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Microstructure, mechanical properties, and elevated-temperature (below the glass transition temperature) tribological performance of the activated combustion-high velocity air fuel (AC-HVAF)-sprayed Fe-Cr-Mo-W-C-B-Y amorphous coating (AC) were investigated. In vacuum, the enhanced hardness favored the wear resistance of Fe-based AC as the temperature rose from 293 K to 673 K. Moreover, the wear mechanism was modified from abrasive wear accompanied by delamination and adhesive wear to the delamination and adhesive wear. In air, the oxidation reaction worsened the splat-to-splat bonding and accelerated the wear rate of Fe-based AC at 673 K. Meanwhile, the elevated-temperature wear failure was the delamination, adhesive, and intensified oxidative wear. Fe-based AC exhibited superior elevated-temperature wear resistance, demonstrating its significant prospect as a wear-resistant coating material for aggressive elevated-temperature applications.
引用
收藏
页数:10
相关论文
共 55 条
[1]   CONTACT AND RUBBING OF FLAT SURFACES [J].
ARCHARD, JF .
JOURNAL OF APPLIED PHYSICS, 1953, 24 (08) :981-988
[2]   On the subsurface deformation of two different Fe-based bulk metallic glasses indented by Vickers micro hardness [J].
Askari-Paykani, Mohsen ;
Nili-Ahmadabadi, Mahmoud ;
Seiffodini, Amir .
INTERMETALLICS, 2014, 46 :118-125
[3]   Elevated-temperature tribology of metallic materials [J].
Blau, Peter J. .
TRIBOLOGY INTERNATIONAL, 2010, 43 (07) :1203-1208
[4]   Effect of tungsten, molybdenum, nickel and cobalt on the corrosion and wear performance of Fe-based metallic glass coatings [J].
Burkov, A. A. ;
Chigrin, P. G. .
SURFACE & COATINGS TECHNOLOGY, 2018, 351 :68-77
[5]   In Situ Synthesis and Characterization of Fe-Based Metallic Glass Coatings by Electrospark Deposition Technique [J].
Burkov, Alexander A. ;
Pyachin, S. A. ;
Ermakov, M. A. ;
Syuy, A. V. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (02) :901-908
[6]   Structure relaxation effect on hardness and shear transformation zone volume of a Ni-Nb metallic glassy film [J].
Chen, H. ;
Song, Y. X. ;
Zhang, T. H. ;
Wu, M. ;
Ma, Y. .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2018, 499 :257-263
[7]   Devitrification of arc-sprayed FeBSiNb amorphous coatings: Effects on wear resistance and mechanical behavior [J].
Cheng, J. B. ;
Liang, X. B. ;
Xu, B. S. .
SURFACE & COATINGS TECHNOLOGY, 2013, 235 :720-726
[8]   Dry sliding friction and wear properties of metallic glass coating and martensite stainless coating [J].
Cheng, J. B. ;
Liang, X. B. ;
Wang, Z. H. ;
Xu, B. S. .
TRIBOLOGY INTERNATIONAL, 2013, 60 :140-146
[9]   Wear Behaviors of Arc-Sprayed FeBSiNb Amorphous Coatings [J].
Cheng, Jiangbo ;
Liu, Dan ;
Liang, Xiubing ;
Chen, Yongxiong .
TRIBOLOGY LETTERS, 2015, 60 (02)
[10]   Wear behavior of Er-bearing Cu-based amorphous/crystal BMG composite under oil lubrication [J].
Chou, Chau-Chang ;
Wang, Shing-Hoa ;
Chung, Hsien-Hung ;
Liaw, Peter K. ;
Liou, Yung ;
Huang, J. C. ;
Hsu, Yuan-Yi .
INTERMETALLICS, 2011, 19 (08) :1216-1221