Novel light-weight glass-ceramic proppants based on frits for hydraulic fracturing process

被引:21
作者
Abd El-Kader, M. [1 ]
Abdou, M., I [2 ]
Fadl, A. M. [2 ]
Abd Rabou, A. [1 ]
Desouky, O. A. [3 ]
El-Shahat, M. F. [4 ]
机构
[1] Arkan Mfg & Min Co, 10th Of Ramdan City, Egypt
[2] EPRI, Prod Dept, Cairo, Egypt
[3] BHIE, Bilbeis Sharqyia, Egypt
[4] Ain Shams Univ, Fac Sci, Cairo, Egypt
关键词
Ceramic proppants; Frit; Egyptian ores; Crushing resistance; Glaze; CRYSTALLIZATION;
D O I
10.1016/j.ceramint.2019.09.173
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
High strength proppants were always in demand for hydraulic fracturing techniques used in unconventional reservoirs for oil and gas extraction processes. To support this concept, relatively low-alumina content glass-ceramic proppants based on the system Fe2O3-TiO2-MgO-CaO-SiO2-Al2O3 have been prepared by using frit, kaolin, and bentonite in a glaze formulation. By deposition of glaze drops on porous ceramic file, a semi-dry proppant beads were obtained. Different frit compositions of aluminum oxide replacing calcium oxide were used to obtain highly sintered proppants with a robust glassy matrix at 1100 degrees C in a fast firing cycle. The microstructure by scanning electron microscopy (SEM) and the phase structure by X-ray diffraction (XRD) were investigated. The results revealed the formation of two main phases; cristobalite and calcium aluminum silicate in addition to the other two phases of mullite and Diopside ferrian in some samples. By evaluating the employed fabricated ceramic compositions as high conductivity and high strength proppants for hydraulic fracturing process it was found that all samples exhibited competitive properties according to American Petroleum Institute standards (API RP 19C Standard) for proppants criteria. Crushing loss under 7500 psi closed pressure was (from 1.5% to 6.7%), the weight loss by acids attack was (from 0.001% to 0.07%), sphericity and roundness were (0.9) in addition, the apparent and bulk densities were (from 2.51 to 2.58 g/cm(3)) and (from 1.46 to 1.50 g/cm(3)), respectively.
引用
收藏
页码:1947 / 1953
页数:7
相关论文
共 25 条
[1]   The Egyptian kaolin: an outlook in the view of the new climate of investment [J].
Abdel-Khalek, NA .
APPLIED CLAY SCIENCE, 1999, 15 (3-4) :325-336
[2]   Sintered esseneite-wollastonite-plagioclase glass-ceramics from vitrified waste [J].
Bernardo, E. ;
Esposito, L. ;
Rambaldi, E. ;
Tucci, A. ;
Pontikes, Y. ;
Angelopoulos, G. N. .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2009, 29 (14) :2921-2927
[3]  
Campos V. P. P. de, 2018, Cerâmica, V64, P219
[4]  
Fadl A.M., 2019, GLOB J ENV SCI, V2, P1
[5]   Synthesis and microstructural evolution in iron oxide kaolinite based proppant as a function of reducing atmosphere, sintering conditions, and composition [J].
Han, Kyu-Bum ;
Graser, Jake ;
Robert, Christian J. ;
de Mendonca Filho, Laercio Martins ;
McLennan, John ;
Sparks, Taylor D. .
CERAMICS INTERNATIONAL, 2018, 44 (08) :9976-9983
[6]   Low-temperature sintering of ceramic proppants by adding solid wastes [J].
Hao, Jianying ;
Ma, Haiqiang ;
Feng, Xin ;
Gao, Yunfeng ;
Wang, Kaiyue ;
Tian, Yuming .
INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2018, 15 (02) :563-568
[7]   Mechanics of light weight proppants: A discrete approach [J].
Kulkarni, M. C. ;
Ochoa, O. O. .
COMPOSITES SCIENCE AND TECHNOLOGY, 2012, 72 (08) :879-885
[8]  
Liang F., 2016, Petroleum, V2, P26, DOI [DOI 10.1016/J.PETLM.2015.11.001, 10.1016/j.petlm.2015.11, DOI 10.1016/J.PETLM.2015.11]
[9]   Low-temperature sintering of bauxite-based fracturing proppants containing CaO and MnO2 additives [J].
Liu, Zuolei ;
Zhao, Jinzhou ;
Li, Yongming ;
Zeng, Zhaohong ;
Mao, Jincheng ;
Peng, Yu ;
He, Yun .
MATERIALS LETTERS, 2016, 171 :300-303
[10]   Study and characterization of pyroxene-based glass-ceramic glazes. [J].
Lucas, F ;
Belda, A ;
Torres, FJ ;
Alarcón, J .
BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 2004, 43 (05) :849-854