Adjust dilution level to suppress the precipitated phase by dilution level model of dissimilar metal laser welding with filler wire

被引:9
作者
Cheng, Bo [1 ]
Wu, Dongjiang [1 ]
Liu, Jun [1 ]
Cui, Qiang [1 ]
Zhou, Siyu [2 ]
Ma, Guangyi [1 ]
Niu, Fangyong [1 ]
机构
[1] Dalian Univ Technol, Key Lab Precis & Nontradit Machining Technol, Minist Educ, Dalian 116024, Liaoning, Peoples R China
[2] Shengyang Aerosp Univ, Sch Mechatron Engn, Shenyang 110136, Liaoning, Peoples R China
关键词
Dilution level; Laser welding; Filler wire; Dissimilar metal; Nickel-based alloy; Precipitated phase; MECHANICAL-PROPERTIES; STAINLESS-STEELS; BEAD GEOMETRY; INTERCRYSTALLINE CORROSION; ALLOY; SOLIDIFICATION; PARAMETERS; SURFACE; COPPER;
D O I
10.1016/j.optlastec.2019.106025
中图分类号
O43 [光学];
学科分类号
070207 ; 0803 ;
摘要
To suppress the precipitated phase by adjusting the dilution level of 304 in the dissimilar metal (Hastelloy C-276/SUS 304) laser welding with filler wire, a mathematical model was established between laser parameters and the dilution level of 304 through energy conservation and mass conservation. And the model was verified by the corresponding experiment. The dilution level of 304 is linear with the single pulse energy E and inverse of wire feeding speed (1/V-F), and it is also affected by energy melting efficiency and the ratio of two base metals melting. The dilution level of 304 is positively correlated with energy melting efficiency and negatively correlated with the ratio of two base metals melting. Defocusing distance and pulse width can affect dilution level of 304 by changing energy melting efficiency. Welding speed and laser beam offset can affect dilution level of 304 by changing the ratio of two base metals melting. At the same time, the influencing mechanism of the dilution level of 304 on the precipitated phase is revealed. The precipitated phase is directly related to the dilution level of 304. With the increase of dilution level of 304, the volume fraction of precipitated phase increases first and then decreases. When the dilution level of 304 is 24.0% similar to 35.2%, the volume fraction of precipitated phase is the biggest. And when the dilution level of 304 arrives to about 73.0%, the precipitated phase approximately disappears. As the result, the dilution level of 304 can be adjusted to suppress the precipitated phase by the dilution model in the laser welding Hastelloy C-276/SUS 304 with filler wire.
引用
收藏
页数:11
相关论文
共 34 条
[11]  
Coniglio N, 2008, WELD J, V87, p237S
[12]   Modeling and optimization of features of bead geometry including percentage dilution in submerged arc welding using mixture of fresh flux and fused slag [J].
Datta, Saurav ;
Bandyopadhyay, Asish ;
Pal, Pradip Kumar .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2008, 36 (11-12) :1080-1090
[13]  
DUPONT JN, 1995, WELD J, V74, pS406
[14]   Dilution in single pass arc welds [J].
DuPont, JN ;
Marder, AR .
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 1996, 27 (03) :481-489
[15]   Effect of steel to aluminum laser welding parameters on mechanical properties of weld beads [J].
Guan Qianqian ;
Long Jiangqi ;
Yu Ping ;
Jiang Shunchao ;
Huang Wenhao ;
Zhou Jianxi .
OPTICS AND LASER TECHNOLOGY, 2019, 111 :387-394
[16]   The influence of dilution on dissimilar weld joints with high-alloy TRIP/TWIP steels [J].
Halbauer, Lars ;
Buchwalder, Anja ;
Zenker, Rolf ;
Biermann, Horst .
WELDING IN THE WORLD, 2016, 60 (04) :645-652
[17]   Microstructure and mechanical properties of laser welded TC4 titanium alloy/304 stainless steel joint with (CoCrFeNi)100-xCux high-entropy alloy interlayer [J].
Hao, Xiaohu ;
Dong, Honggang ;
Xia, Yueqing ;
Li, Peng .
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 803 :649-657
[18]   Intercrystalline corrosion of surface-welds of nickel alloys on carbon steel [J].
Huerta, D ;
Siefert, B .
JOURNAL OF MATERIALS SCIENCE, 2005, 40 (19) :5153-5159
[19]   Influence of heating source position and dilution rate in achieving overmatched dissimilar welded joints [J].
Iordachescu, M. ;
Iordachescu, D. ;
Scutelnicu, E. ;
Ruiz-Hervias, J. ;
Valiente, A. ;
Caballero, L. .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2010, 15 (05) :378-385
[20]   Development of a chromium-free consumable for austenitic stainless steels: Effect of dilution and the behavior of bead-on-plate welds [J].
Kim, Yeong Ho ;
Frankel, G. S. ;
Lippold, J. C. .
ISIJ INTERNATIONAL, 2006, 46 (05) :698-704